Analyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopy

(Na0.55K0.45)NbO3 (NKN) and acceptor-doped (Na0.55K0.45)(Nb1-xZr5x/4)O3 (NKNZ; x = 0.005 and 0.01) piezoelectric ceramics were fabricated by the conventional solid-state reaction method. Both ceramics were applied to a fatigue test for 106 cycles under an electric field at 3 kV/mm with unipolar driv...

Full description

Bibliographic Details
Main Authors: Kiyotaka Tanaka, Sayaka Takatsuka, Hiroshi Nishiyama, Ken-ichi Kakimoto
Format: Article
Language:English
Published: AIP Publishing LLC 2019-04-01
Series:AIP Advances
Online Access:http://dx.doi.org/10.1063/1.5089533
_version_ 1819088199907016704
author Kiyotaka Tanaka
Sayaka Takatsuka
Hiroshi Nishiyama
Ken-ichi Kakimoto
author_facet Kiyotaka Tanaka
Sayaka Takatsuka
Hiroshi Nishiyama
Ken-ichi Kakimoto
author_sort Kiyotaka Tanaka
collection DOAJ
description (Na0.55K0.45)NbO3 (NKN) and acceptor-doped (Na0.55K0.45)(Nb1-xZr5x/4)O3 (NKNZ; x = 0.005 and 0.01) piezoelectric ceramics were fabricated by the conventional solid-state reaction method. Both ceramics were applied to a fatigue test for 106 cycles under an electric field at 3 kV/mm with unipolar drive. After the fatigue test, the maximum polarization of NKN and NKNZ (x = 0.005) was decreased by approximately 15 and 5%, respectively. Therefore, we found that the fatigue resistance properties of NKNZ ceramics, which substituted the Nb5+ ion with the Zr4+ ion, were improved. To study fatigue phenomena in piezoelectric ceramics, the chemical bond strength of both ceramics before and after the fatigue test was analyzed by soft X-ray emission spectroscopy (SXES), which has high energy resolution and is suitable for the evaluation of light elements in a local region with the micrometer order. We evaluated the formation of oxygen vacancies in as-sintered, poled, and fatigued ceramics by analyzing a chemical shift of the O Ka(3) peak appeared at approximately 175 eV in the SXES spectra. In NKN ceramics, the O Ka(3) peak was shifted to the higher energy side by the poling treatment and fatigue test. The peak position of fatigued NKN ceramics was close to that of the standard SrTiO3 sample. It was considered that the oxygen vacancies of the fatigued NKN ceramics had accumulated at grain boundaries instead of the oxygen moving. The improvement of the fatigue resistance for the NKNZ ceramics was attributed to the formation of a defect dipole connected with the oxygen vacancy and acceptor Zr ion.
first_indexed 2024-12-21T21:48:15Z
format Article
id doaj.art-ab5b56952a55419bb1487eaa1f6d723c
institution Directory Open Access Journal
issn 2158-3226
language English
last_indexed 2024-12-21T21:48:15Z
publishDate 2019-04-01
publisher AIP Publishing LLC
record_format Article
series AIP Advances
spelling doaj.art-ab5b56952a55419bb1487eaa1f6d723c2022-12-21T18:49:09ZengAIP Publishing LLCAIP Advances2158-32262019-04-0194045102045102-610.1063/1.5089533114903ADVAnalyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopyKiyotaka Tanaka0Sayaka Takatsuka1Hiroshi Nishiyama2Ken-ichi Kakimoto3Technical Division, Nagoya Institute of Technology, Nagoya 466-8555, JapanDepartment of Life Science and Applied Chemistry, Nagoya Institute of Technology, Nagoya 466-8555, JapanDepartment of Life Science and Applied Chemistry, Graduate School of Engineering, Nagoya Institute of Technology, Nagoya 466-8555, JapanDepartment of Life Science and Applied Chemistry, Nagoya Institute of Technology, Nagoya 466-8555, Japan(Na0.55K0.45)NbO3 (NKN) and acceptor-doped (Na0.55K0.45)(Nb1-xZr5x/4)O3 (NKNZ; x = 0.005 and 0.01) piezoelectric ceramics were fabricated by the conventional solid-state reaction method. Both ceramics were applied to a fatigue test for 106 cycles under an electric field at 3 kV/mm with unipolar drive. After the fatigue test, the maximum polarization of NKN and NKNZ (x = 0.005) was decreased by approximately 15 and 5%, respectively. Therefore, we found that the fatigue resistance properties of NKNZ ceramics, which substituted the Nb5+ ion with the Zr4+ ion, were improved. To study fatigue phenomena in piezoelectric ceramics, the chemical bond strength of both ceramics before and after the fatigue test was analyzed by soft X-ray emission spectroscopy (SXES), which has high energy resolution and is suitable for the evaluation of light elements in a local region with the micrometer order. We evaluated the formation of oxygen vacancies in as-sintered, poled, and fatigued ceramics by analyzing a chemical shift of the O Ka(3) peak appeared at approximately 175 eV in the SXES spectra. In NKN ceramics, the O Ka(3) peak was shifted to the higher energy side by the poling treatment and fatigue test. The peak position of fatigued NKN ceramics was close to that of the standard SrTiO3 sample. It was considered that the oxygen vacancies of the fatigued NKN ceramics had accumulated at grain boundaries instead of the oxygen moving. The improvement of the fatigue resistance for the NKNZ ceramics was attributed to the formation of a defect dipole connected with the oxygen vacancy and acceptor Zr ion.http://dx.doi.org/10.1063/1.5089533
spellingShingle Kiyotaka Tanaka
Sayaka Takatsuka
Hiroshi Nishiyama
Ken-ichi Kakimoto
Analyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopy
AIP Advances
title Analyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopy
title_full Analyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopy
title_fullStr Analyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopy
title_full_unstemmed Analyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopy
title_short Analyses for oxygen vacancies in (Na,K)NbO3-series piezoelectric ceramics by soft x-ray emission spectroscopy
title_sort analyses for oxygen vacancies in na k nbo3 series piezoelectric ceramics by soft x ray emission spectroscopy
url http://dx.doi.org/10.1063/1.5089533
work_keys_str_mv AT kiyotakatanaka analysesforoxygenvacanciesinnaknbo3seriespiezoelectricceramicsbysoftxrayemissionspectroscopy
AT sayakatakatsuka analysesforoxygenvacanciesinnaknbo3seriespiezoelectricceramicsbysoftxrayemissionspectroscopy
AT hiroshinishiyama analysesforoxygenvacanciesinnaknbo3seriespiezoelectricceramicsbysoftxrayemissionspectroscopy
AT kenichikakimoto analysesforoxygenvacanciesinnaknbo3seriespiezoelectricceramicsbysoftxrayemissionspectroscopy