Recipe of Lightweight Slurry with High Early Strength of the Resultant Cement Sheath
Admixtures of mineral or waste filling materials are used to reduce slurry density. However, the sheath made of lightweight cement slurry has low mechanical performance at the initial bonding time. The required strength is achieved later. This is the main problem when evaluating the cement bond logg...
Main Author: | Marcin Kremieniewski |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2020-04-01
|
Series: | Energies |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1073/13/7/1583 |
Similar Items
-
Ultra-Lightweight Cement Slurry to Seal Wellbore of Poor Wellbore Stability
by: Marcin Kremieniewski
Published: (2020-06-01) -
Lightweight cement mortar with inorganic perlite microspheres for equipping oil and gas production wells
by: O.V. Kazmina, et al.
Published: (2020-02-01) -
CEMENT SLURRIES FOR GEOTHERMAL WELLS CEMENTING
by: Nediljka Gaurina-Međimurec, et al.
Published: (1994-12-01) -
Reduction of Fractionation of Lightweight Slurry to Geothermal Boreholes
by: Marcin Kremieniewski, et al.
Published: (2021-06-01) -
A novel predictive model for the compressive strength development in class G cement slurries at different temperatures, retarder, and salt concentrations
by: Ali Barati Harooni, et al.
Published: (2025-07-01)