Study of Short Times Tempering for AISI D2 Cold Work Tool Steel
Short time tempering has been applied to steels to improve toughness keeping the hardness at the same level. For AISI D2 tool steel, typical thermal cycles are quench and temper. The austenitizing temperature is around 1040 ºC and the subsequent double tempering at temperatures close to 500 ºC, for...
Main Authors: | Maycoln D. Conci, Dany M.A. Centeno, Hélio Goldenstein, Paula F.S. Farina |
---|---|
Format: | Article |
Language: | English |
Published: |
Associação Brasileira de Metalurgia e Materiais (ABM); Associação Brasileira de Cerâmica (ABC); Associação Brasileira de Polímeros (ABPol)
2023-09-01
|
Series: | Materials Research |
Subjects: | |
Online Access: | http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392023000200262&tlng=en |
Similar Items
-
Hardness Prediction in Quenched and Tempered Nodular Cast Iron Using the Hollomon-Jaffe Parameter
by: Fidel Salas Vicente, et al.
Published: (2021-02-01) -
The Effect of Deep Cryogenic Processing and Tempering Heat Treatment of AISI H13 Tool Steel on Microstructure, Hardness and Impact Energy
by: Melika ÖZER
Published: (2019-09-01) -
Mechanical Properties and Microstructure Characterization of AISI “D2” and “O1” Cold Work Tool Steels
by: Mohammed Algarni
Published: (2019-10-01) -
Effect of spheroidized microstructure on quenching and tempering characteristics and corrosion resistance of AISI 420-type steel
by: LÜ Chuan-jiang, et al.
Published: (2019-09-01) -
Microstructural variations and mechanical properties of deep cryogenic treated AISI M35 high-speed steel tempered at various temperatures
by: Guili Xu, et al.
Published: (2022-03-01)