The Combined Influence of Molybdenum and Nickel in Steel Welds
Weld metal deposit (WMD) was carried out for standard MMA welding process. This welding method is still promising mainly due to the high amount of AF (acicular ferrite) and low amount of MAC (self-tempered martensite, retained austenite, carbide) phases in WMD. That structure corresponds with good i...
Main Authors: | B. Szczucka-Lasota, T. Węgrzyn, A. Kurc-Lisiecka, J. Piwnik |
---|---|
Format: | Article |
Language: | English |
Published: |
Polish Academy of Sciences
2018-10-01
|
Series: | Archives of Metallurgy and Materials |
Subjects: | |
Online Access: | https://journals.pan.pl/Content/107983/AMM-2018-3-03-Wegrzyn.pdf |
Similar Items
-
Low Alloy Steel Structures After Welding with Micro-Jet Cooling
by: Węgrzyn T., et al.
Published: (2017-03-01) -
Impact Toughness of Steel WMD After TIG Welding
by: Węgrzyn T., et al.
Published: (2017-09-01) -
Effect of welding parameters on microstructure and properties of friction stir welded joints for ferritic stainless steel
by: TANG Wen-shen, et al.
Published: (2019-05-01) -
Micro-jet Cooling by Compressed Air after MAG Welding
by: Węgrzyn T., et al.
Published: (2016-06-01) -
The Use of Compressed Air for Micro-Jet Cooling After MIG Welding
by: Hadryś D., et al.
Published: (2016-09-01)