Effects of severe plastic deformation on the magnetic properties of terbium
We report on the magnetic and magnetocaloric properties of Terbium ribbons subjected by cold rolling. The magnetic entropy change ΔS = 8.66 J/(kg·K) and adiabatic temperature change ΔT = 4.38 K for a bulk sample of Terbium in an external magnetic field change of 1.9 T are larger by about 12% and 26%...
Main Authors: | S. Taskaev, K. Skokov, V. Khovaylo, D. Karpenkov, M. Ulyanov, D. Bataev, A. Dyakonov, O. Gutfleisch |
---|---|
Format: | Article |
Language: | English |
Published: |
AIP Publishing LLC
2018-04-01
|
Series: | AIP Advances |
Online Access: | http://dx.doi.org/10.1063/1.4998292 |
Similar Items
-
Magnetic properties and magnetocaloric effect in Dy100-xYx solid solutions
by: Sergey Taskaev, et al.
Published: (2021-01-01) -
Coherent magnetic structures in terbium/holmium superlattices
by: BrynJacobsen, C, et al.
Published: (1997) -
Magnetic dilution by severe plastic deformation
by: Martin Stückler, et al.
Published: (2020-01-01) -
Analysis of the Magnetocaloric Effect in Heusler Alloys: Study of Ni50CoMn36Sn13 by Calorimetric Techniques
by: Elias Palacios, et al.
Published: (2015-03-01) -
Thermodynamic Properties of Terbium Tellurides
by: Samira Z. Imamaliyeva, et al.
Published: (2020-12-01)