Electrophoretic deposition and thermal treatment of boehmite coatings on titanium
An aqueous boehmite sol was prepared by the peptization of Al(OH)3. The electrophoretic deposition of boehmite coatings on titanium from the aqueous sol was performed at a constant voltage (from 1.0 to 10 V) and for a constant deposition time (from 10 to 30 min). Increasing the applied voltage and d...
Main Authors: | Đošić Marija S., Mišković-Stanković Vesna B., Srdić Vladimir V. |
---|---|
Format: | Article |
Language: | English |
Published: |
Serbian Chemical Society
2007-01-01
|
Series: | Journal of the Serbian Chemical Society |
Subjects: | |
Online Access: | http://www.doiserbia.nb.rs/img/doi/0352-5139/2007/0352-51390703275D.pdf |
Similar Items
-
Electrophoretic deposition and thermal treatment of boehmite coatings on titanium
by: MARIJA S. DJOSIC, et al.
Published: (2007-03-01) -
Electrophoretic deposition of alumina and boehmite coatings on metal surfaces
by: Vesna Miskovic-Stankovic
Published: (2012-12-01) -
Influence of boehmite intermediate layer as covalent linker on synthesis of LTA zeolite coatings
by: Leidys Marleyn Rodríguez-Castro, et al.
Published: (2020-06-01) -
Electrophoretic Deposition of Biocompatible and Bioactive Hydroxyapatite-Based Coatings on Titanium
by: Marija Djošić, et al.
Published: (2021-09-01) -
Electrophoretically deposited hydroxyapatite-based composite coatings loaded with silver and gentamicin as antibacterial agents
by: Stevanović Milena, et al.
Published: (2019-01-01)