Characterization of friction stir welded Al-4Cu-Mg alloy / Al-16Si-4Cu-10SiC composite joint
This study investigated the tool's rotational speed effect during dissimilar friction stir welding of A390–10 wt.% SiC composite-AA2024 aluminum alloy on microstructure, mechanical properties, and corrosion resistance. The results show that the tunnel defect is created on the advancing side at...
Main Authors: | Hamed Jamshidi Aval, Ivan Galvão |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2024-06-01
|
Series: | Journal of Advanced Joining Processes |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2666330924000098 |
Similar Items
-
Microstructural characterization and corrosion-resistance behavior of friction stir-welded A390/10 wt% SiC composites-AA2024 Al alloy joints
by: Hamed Jamshidi Aval, et al.
Published: (2024-04-01) -
Dissimilar Friction Stir Welding of AA2024 and AISI 1018: Microstructure and Mechanical Properties
by: Mohamed M. Z. Ahmed, et al.
Published: (2021-02-01) -
Microstructure and Mechanical Properties of Dissimilar Friction Stir Welded AA2024-T4/AA7075-T6 T-Butt Joints
by: Mohamed M.Z. Ahmed, et al.
Published: (2021-01-01) -
Fabrication Of Al 2024/SiC Nanocomposite with Al and Cu Pure Coatings
by: P. Melali, et al.
Published: (2015-06-01) -
An overview of friction stir processing of Cu–SiC composites: Microstructural, mechanical, tribological, and electrical properties
by: Mohammad Reza Akbarpour, et al.
Published: (2023-11-01)