Surface roughness and microhardness of enamel white spot lesions treated with different treatment methods
Objective: To analyse the surface roughness and microhardness of artificial enamel white spot lesions before and after WSL formation, after treatment (Opalsutre™ microabrasion, Sylc® bioactive glass, and ICON® resin infiltration), and after pH cycling with the help of the profilometer surface roughn...
Main Authors: | Mina MG. Chabuk, Abdulla MW. Al-Shamma |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2023-07-01
|
Series: | Heliyon |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2405844023054919 |
Similar Items
-
Management Of Clear Aligner-related Severe Enamel Demineralization With A Modified Resin Infiltration Technique: A Case Report
by: Vo Truong Nhu Ngoc, et al.
Published: (2023-01-01) -
Real-Time Monitoring and Quantitative Evaluation of Resin In-Filtrant Repairing Enamel White Spot Lesions Based on Optical Coherence Tomography
by: Sujuan Zeng, et al.
Published: (2021-11-01) -
Microhardness and surface roughness of resin infiltrated bleached enamel surface using atomic force microscopy: An in vitro study
by: Alaa M. Alsafi, et al.
Published: (2023-09-01) -
Spectrophotometric Evaluation of Enamel Color Variation Using Infiltration Resin Treatment of White Spot Lesions at One Year Follow-Up
by: Roberto Lo Giudice, et al.
Published: (2020-04-01) -
Long-Term Chromatic Durability of White Spot Lesions through Employment of Infiltration Resin Treatment
by: Francesco Puleio, et al.
Published: (2023-04-01)