Hot Deformation Behavior and Microstructure Evolution of Cu–Ni–Co–Si Alloys
The Cu-1.7Ni-1.4Co-0.65Si (wt%) alloy is hot compressed by a Gleeble-1500D machine under a temperature range of 760 to 970 °C and a strain rate range of 0.01 to 10 s<sup>−1</sup>. The flow stress increases with the extension of strain rate and decreases with the rising of deformation tem...
Main Authors: | Feng Liu, Jimiao Ma, Lijun Peng, Guojie Huang, Wenjing Zhang, Haofeng Xie, Xujun Mi |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2020-04-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/13/9/2042 |
Similar Items
-
Microstructure Analysis and Segmented Constitutive Model for Ni-Cr-Co-Based Superalloy during Hot Deformation
by: Hongyu Li, et al.
Published: (2022-02-01) -
Microstructure of Hot-Deformed Cu-3Ti Alloy
by: Szkliniarz A., et al.
Published: (2016-03-01) -
Effects of Co Addition on the Microstructure and Properties of Elastic Cu-Ni-Si-Based Alloys for Electrical Connectors
by: Zheng Wang, et al.
Published: (2021-04-01) -
Exploring hot deformation behavior of the solutionized Cu–15Ni–8Sn alloy through constitutive equations and processing maps
by: Xuemao Dong, et al.
Published: (2024-03-01) -
Hot Deformation and Dynamic Recrystallization Behavior of CoCrNi and (CoCrNi)<sub>94</sub>Ti<sub>3</sub>Al<sub>3</sub> Medium Entropy Alloys
by: Hai-long Yi, et al.
Published: (2020-10-01)