Repair Welding of the Massive Cast

The rebuilding technologies are used to develop surface of ladle. Among many welding methods currently used to obtain surface layer without defects one of the most effective way of rebuilding is using metal arc welding. This additional material gives more possibilities to make expected quality of re...

Full description

Bibliographic Details
Main Author: Bęczkowski R.
Format: Article
Language:English
Published: Polish Academy of Sciences 2017-06-01
Series:Archives of Foundry Engineering
Subjects:
Online Access:http://www.degruyter.com/view/j/afe.2017.17.issue-2/afe-2017-0041/afe-2017-0041.xml?format=INT
_version_ 1797720578193358848
author Bęczkowski R.
author_facet Bęczkowski R.
author_sort Bęczkowski R.
collection DOAJ
description The rebuilding technologies are used to develop surface of ladle. Among many welding methods currently used to obtain surface layer without defects one of the most effective way of rebuilding is using metal arc welding. This additional material gives more possibilities to make expected quality of rebuild surface. Chemical composition, property and economic factors allow to use metal wire. Because of these reasons, solid wire gives opportunity to be wildly used as material to rebuild or repair the surface in different sectors of industry. The paper shows a few ways to rebuild the surface in the massive cast with the use of metal active gas welding for repair. The work presents studies of defect in the massive cast. It contains the pictures of microstructures and defects. The method of removing defects and the results of checking by visual and penetrant testing methods are shown. The paper describes the methodology of repair the ladle with metal active gas welding, preheating process and standards nondestructive testing method.
first_indexed 2024-03-12T09:22:31Z
format Article
id doaj.art-be66dab6a9204706b3a927d257f1283f
institution Directory Open Access Journal
issn 2299-2944
language English
last_indexed 2024-03-12T09:22:31Z
publishDate 2017-06-01
publisher Polish Academy of Sciences
record_format Article
series Archives of Foundry Engineering
spelling doaj.art-be66dab6a9204706b3a927d257f1283f2023-09-02T14:26:34ZengPolish Academy of SciencesArchives of Foundry Engineering2299-29442017-06-011725810.1515/afe-2017-0041afe-2017-0041Repair Welding of the Massive CastBęczkowski R.0Institute of Mechanical Technology, Czestochowa University of Technology, 21 Armii Krajowej Av., 42-201 Czestochowa, PolandThe rebuilding technologies are used to develop surface of ladle. Among many welding methods currently used to obtain surface layer without defects one of the most effective way of rebuilding is using metal arc welding. This additional material gives more possibilities to make expected quality of rebuild surface. Chemical composition, property and economic factors allow to use metal wire. Because of these reasons, solid wire gives opportunity to be wildly used as material to rebuild or repair the surface in different sectors of industry. The paper shows a few ways to rebuild the surface in the massive cast with the use of metal active gas welding for repair. The work presents studies of defect in the massive cast. It contains the pictures of microstructures and defects. The method of removing defects and the results of checking by visual and penetrant testing methods are shown. The paper describes the methodology of repair the ladle with metal active gas welding, preheating process and standards nondestructive testing method.http://www.degruyter.com/view/j/afe.2017.17.issue-2/afe-2017-0041/afe-2017-0041.xml?format=INTCast defectRebuildingQualityMAGWelding
spellingShingle Bęczkowski R.
Repair Welding of the Massive Cast
Archives of Foundry Engineering
Cast defect
Rebuilding
Quality
MAG
Welding
title Repair Welding of the Massive Cast
title_full Repair Welding of the Massive Cast
title_fullStr Repair Welding of the Massive Cast
title_full_unstemmed Repair Welding of the Massive Cast
title_short Repair Welding of the Massive Cast
title_sort repair welding of the massive cast
topic Cast defect
Rebuilding
Quality
MAG
Welding
url http://www.degruyter.com/view/j/afe.2017.17.issue-2/afe-2017-0041/afe-2017-0041.xml?format=INT
work_keys_str_mv AT beczkowskir repairweldingofthemassivecast