The influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steel

Characteristics of air hardening steel are high hardness and low impact toughness. In order to increase the impact toughness while retaining high hardness value, studies were performed. One of the ways to achieve this is the alloying of specified steel with vanadium and application of appropriate he...

Full description

Bibliographic Details
Main Authors: Todić Aleksandar, Čikara Dejan, Todić Tomislav, Pejović Branko, Čamagić Ivica, Vukojević Vukoje
Format: Article
Language:English
Published: University of Belgrade - Faculty of Mechanical Engineering, Belgrade 2017-01-01
Series:FME Transactions
Subjects:
Online Access:https://scindeks-clanci.ceon.rs/data/pdf/1451-2092/2017/1451-20921701130T.pdf
_version_ 1828877541108088832
author Todić Aleksandar
Čikara Dejan
Todić Tomislav
Pejović Branko
Čamagić Ivica
Vukojević Vukoje
author_facet Todić Aleksandar
Čikara Dejan
Todić Tomislav
Pejović Branko
Čamagić Ivica
Vukojević Vukoje
author_sort Todić Aleksandar
collection DOAJ
description Characteristics of air hardening steel are high hardness and low impact toughness. In order to increase the impact toughness while retaining high hardness value, studies were performed. One of the ways to achieve this is the alloying of specified steel with vanadium and application of appropriate heat treatment. Vanadium affects the solidification process of these alloys by narrowing of the temperature interval of crystallization. In addition, vanadium formed V6C5 carbides that block the growth of austenitic dendrites and structure makes fine-grained. Vanadium which forms V6C5 carbides is partly distributed between present phases in the steel; carbide (Cr,Fe)7C3 and austenite. Also, the presence of vanadium can enables the formation of (Cr,Fe)23C6 carbide and its precipitation in austenite during the cooling process. In local areas around fine carbide particles, austenite is transformed into martensite. In other words, vanadium reduces the amount of remained austenite and thus improves hardenbility ot the steel. In this way, better technical characteristics of these steels are obtained.
first_indexed 2024-12-13T08:42:57Z
format Article
id doaj.art-bf36fb7be45a422b98fee6ec1f3508e4
institution Directory Open Access Journal
issn 1451-2092
2406-128X
language English
last_indexed 2024-12-13T08:42:57Z
publishDate 2017-01-01
publisher University of Belgrade - Faculty of Mechanical Engineering, Belgrade
record_format Article
series FME Transactions
spelling doaj.art-bf36fb7be45a422b98fee6ec1f3508e42022-12-21T23:53:30ZengUniversity of Belgrade - Faculty of Mechanical Engineering, BelgradeFME Transactions1451-20922406-128X2017-01-014511301341451-20921701130TThe influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steelTodić Aleksandar0Čikara Dejan1Todić Tomislav2Pejović Branko3Čamagić Ivica4Vukojević Vukoje5University of Pristina, Faculty of Technical SciencesUniversity of Pristina, Faculty of Technical SciencesUniversity of Pristina, Faculty of Technical SciencesUniversity of Pristina, Faculty of Technical SciencesUniversity of Pristina, Faculty of Technical SciencesUniversity of Pristina, Faculty of Technical SciencesCharacteristics of air hardening steel are high hardness and low impact toughness. In order to increase the impact toughness while retaining high hardness value, studies were performed. One of the ways to achieve this is the alloying of specified steel with vanadium and application of appropriate heat treatment. Vanadium affects the solidification process of these alloys by narrowing of the temperature interval of crystallization. In addition, vanadium formed V6C5 carbides that block the growth of austenitic dendrites and structure makes fine-grained. Vanadium which forms V6C5 carbides is partly distributed between present phases in the steel; carbide (Cr,Fe)7C3 and austenite. Also, the presence of vanadium can enables the formation of (Cr,Fe)23C6 carbide and its precipitation in austenite during the cooling process. In local areas around fine carbide particles, austenite is transformed into martensite. In other words, vanadium reduces the amount of remained austenite and thus improves hardenbility ot the steel. In this way, better technical characteristics of these steels are obtained.https://scindeks-clanci.ceon.rs/data/pdf/1451-2092/2017/1451-20921701130T.pdfvanadiumimpact toughnesshardnessmicrostructure
spellingShingle Todić Aleksandar
Čikara Dejan
Todić Tomislav
Pejović Branko
Čamagić Ivica
Vukojević Vukoje
The influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steel
FME Transactions
vanadium
impact toughness
hardness
microstructure
title The influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steel
title_full The influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steel
title_fullStr The influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steel
title_full_unstemmed The influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steel
title_short The influence of the vanadium content on the toughness and hardness of wear resistant high-alloyed Cr-Mo steel
title_sort influence of the vanadium content on the toughness and hardness of wear resistant high alloyed cr mo steel
topic vanadium
impact toughness
hardness
microstructure
url https://scindeks-clanci.ceon.rs/data/pdf/1451-2092/2017/1451-20921701130T.pdf
work_keys_str_mv AT todicaleksandar theinfluenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT cikaradejan theinfluenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT todictomislav theinfluenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT pejovicbranko theinfluenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT camagicivica theinfluenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT vukojevicvukoje theinfluenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT todicaleksandar influenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT cikaradejan influenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT todictomislav influenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT pejovicbranko influenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT camagicivica influenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel
AT vukojevicvukoje influenceofthevanadiumcontentonthetoughnessandhardnessofwearresistanthighalloyedcrmosteel