Cold drawing schedules for RSt 34-2 (1.0034) steel wire for correction of overheating defects and breakless ensuring
The paper’s authors researched the defects correction for RSt 34-2 (1.0034) steel wire, obtained as result of its overheating at 1140...1160 °C. Instead of the re-heat treatment method, the authors proposed five cold drawing, annealing and overheating combination schedules, which ensure the increase...
المؤلفون الرئيسيون: | Anishchenko Oleksandr, Kukhar Volodymyr, Oginskiy Iosyp, Korenko Maryna, Prysiazhnyi Andrii |
---|---|
التنسيق: | مقال |
اللغة: | English |
منشور في: |
EDP Sciences
2021-01-01
|
سلاسل: | E3S Web of Conferences |
الوصول للمادة أونلاين: | https://www.e3s-conferences.org/articles/e3sconf/pdf/2021/60/e3sconf_tpacee2021_06005.pdf |
مواد مشابهة
-
Developing of X65 steel coils making at Steckel mill using thermo-mechanical control process
حسب: Kurpe Oleksandr, وآخرون
منشور في: (2021-01-01) -
Analysis of relation between edging ratio and deformation work done in pre-forming of workpiece by bulk buckling
حسب: Kukhar Volodymyr, وآخرون
منشور في: (2018-01-01) -
A Multiwavelength Approach to Constraining the Merger Properties of ACT-CL J0034.4+0225
حسب: Peter Doze, وآخرون
منشور في: (2024-01-01) -
Pyrazole compound BPR1P0034 with potent and selective anti-influenza virus activity
حسب: Yeh Jiann-Yih, وآخرون
منشور في: (2010-02-01) -
Experimental Research and Method for Calculation of 'Upsetting-with-Buckling' Load at the Impression-Free (Dieless) Preforming of Workpiece
حسب: Kukhar Volodymir, وآخرون
منشور في: (2018-01-01)