Cold drawing schedules for RSt 34-2 (1.0034) steel wire for correction of overheating defects and breakless ensuring

The paper’s authors researched the defects correction for RSt 34-2 (1.0034) steel wire, obtained as result of its overheating at 1140...1160 °C. Instead of the re-heat treatment method, the authors proposed five cold drawing, annealing and overheating combination schedules, which ensure the increase...