Cold drawing schedules for RSt 34-2 (1.0034) steel wire for correction of overheating defects and breakless ensuring

The paper’s authors researched the defects correction for RSt 34-2 (1.0034) steel wire, obtained as result of its overheating at 1140...1160 °C. Instead of the re-heat treatment method, the authors proposed five cold drawing, annealing and overheating combination schedules, which ensure the increase...

Mô tả đầy đủ

Chi tiết về thư mục
Những tác giả chính: Anishchenko Oleksandr, Kukhar Volodymyr, Oginskiy Iosyp, Korenko Maryna, Prysiazhnyi Andrii
Định dạng: Bài viết
Ngôn ngữ:English
Được phát hành: EDP Sciences 2021-01-01
Loạt:E3S Web of Conferences
Truy cập trực tuyến:https://www.e3s-conferences.org/articles/e3sconf/pdf/2021/60/e3sconf_tpacee2021_06005.pdf