Effect of Rolling Temperature and Subsequence Ageing on the Mechanical Properties and Microstructure Evolution of an Al-Cu-Li Alloy
The mechanical properties and microstructure evolution of an Al-Cu-Li alloy sheet processed via hot rolling (HR) (at 400 °C and 500 °C) or cryorolling (CR) (at −100 °C and −190 °C) and subsequence aging at 160 °C for 10 h were investigated. Before aging, the highest ultimate tensile strength of 502...
Main Authors: | Lin Wang, Charlie Kong, Puneet Tandon, Alexander Pesin, Denis Pustovoytov, Hailiang Yu |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2021-05-01
|
Series: | Metals |
Subjects: | |
Online Access: | https://www.mdpi.com/2075-4701/11/6/853 |
Similar Items
-
Mechanical properties and microstructure evolution of an Al–Cu–Li alloy via cross cryorolling
by: Lin Wang, et al.
Published: (2022-12-01) -
Twinning susceptibility of CrCoNi medium entropy alloy to cryogenic temperature during asymmetric rolling
by: Yuze Wu, et al.
Published: (2022-09-01) -
Microstructure and texture evolution of pure nickel during cryorolling and subsequent annealing
by: Zhide Li, et al.
Published: (2023-05-01) -
Effect of Ce Content on the Microstructure and Mechanical Properties of Al-Cu-Li Alloy
by: Xianxian Ding, et al.
Published: (2023-01-01) -
Influence of thermal exposure on the microstructure evolution and mechanical behaviors of an Al-Cu-Li alloy
by: Mingdong Wu, et al.
Published: (2023-03-01)