Reduction of Dewaxing and Sintering Time by Controlling the Particle Size of YSZ Particles for Stereolithography
In ceramic stereolithography, composite “green” bodies must be thermally processed to de-bind organic content and sinter the material. The conventional process for dewaxing and sintering of yttria stabilized zirconia stereolithography components is typically very long. The time and energy cost of th...
Main Authors: | Masaya Takahashi, Fiona Spirrett, Soshu Kirihara |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2022-10-01
|
Series: | Ceramics |
Subjects: | |
Online Access: | https://www.mdpi.com/2571-6131/5/4/59 |
Similar Items
-
High-Speed Alumina Stereolithography
by: Fiona Spirrett, et al.
Published: (2022-09-01) -
Analysis of the Luminescent Emission during Flash Sintering of 8YSZ and 20SDC Ceramics
by: Reginaldo Muccillo, et al.
Published: (2024-02-01) -
Effect of Heating Mode on Sinterability of YSZ+CeO2 Ceramics
by: A. Raja Annamalai, et al.
Published: (2018-03-01) -
Ceramic Stereolithography of Li<sub>7</sub>La<sub>3</sub>Zr<sub>2</sub>O<sub>12</sub> Micro-Embossed Sheets for Solid Electrolyte Applications
by: Fiona Spirrett, et al.
Published: (2024-09-01) -
Phase Formation and the Electrical Properties of YSZ/rGO Composite Ceramics Sintered Using Silicon Carbide Powder Bed
by: Artem Glukharev, et al.
Published: (2021-12-01)