Effects of cooling rate on solidification cracking behaviour in 310S stainless steel
In order to change the cooling rate of weld pool, in-situ laser post-heating was irradiated behind the weld pool during gas tungsten arc welding in a U-type hot cracking test. The solidification cracking occurrence based on the cooling rate change was observed. The high temperature ductility curve a...
Main Authors: | Jae-Hyeong Lee, Shotaro Yamashita, Tomo Ogura, Kazuyoshi Saida |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2021-06-01
|
Series: | Journal of Advanced Joining Processes |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2666330921000042 |
Similar Items
-
Effects of ferrite content and concentrations of carbon and silicon on weld solidification cracking susceptibility of stainless steels
by: Kota Kadoi, et al.
Published: (2023-07-01) -
Solidification cracking nature and sequence of different stainless steels
by: Hsuan-Han Lai, et al.
Published: (2023-07-01) -
Effects of Cerium on Weld Solidification Crack Sensitivity of 441 Ferritic Stainless Steel
by: Shuangchun Zhu, et al.
Published: (2019-03-01) -
Formation condition of lacy ferrite during solidification and subsequent transformation in austenitic stainless steels solidified with primary ferrite
by: Kota Kadoi, et al.
Published: (2024-05-01) -
Predicting Susceptibility to Solidification Cracking and Liquation Cracking by CALPHAD
by: Sindo Kou
Published: (2021-09-01)