Influence of retempering on properties of concrete made with manufactured sand and industrial waste

The construction industry is currently dealing with a number of major issues. These include of shortage of river sand and large amount of energy required for manufacturing of cement produces free CO2 in air, accordingly use of manufactured sand and industrial waste in concrete increases. In construc...

Full description

Bibliographic Details
Main Authors: Kiran M. Mane, Abhay M. Joshi, D.K. Kulkarni, K.B. Prakash
Format: Article
Language:English
Published: Elsevier 2022-06-01
Series:Cleaner Materials
Subjects:
Online Access:http://www.sciencedirect.com/science/article/pii/S277239762200020X
_version_ 1811251559176077312
author Kiran M. Mane
Abhay M. Joshi
D.K. Kulkarni
K.B. Prakash
author_facet Kiran M. Mane
Abhay M. Joshi
D.K. Kulkarni
K.B. Prakash
author_sort Kiran M. Mane
collection DOAJ
description The construction industry is currently dealing with a number of major issues. These include of shortage of river sand and large amount of energy required for manufacturing of cement produces free CO2 in air, accordingly use of manufactured sand and industrial waste in concrete increases. In construction of hilly topography long carrying of concrete is required, In outside location providing of concrete from inner mixing place, in construction of road, in lengthy tunneling work, manual transportation of concrete by labor, directly affect the flow property and concrete get stiff at the time of casting on real site work and in several conditions concrete get rejected by engineers. The paper discusses effects of replacing cement with 20% of industrial waste silica fumes and partially replacing natural sand with manufactured sand in the context of properties of retempered concrete like flow, water absorption, sorptivity, tensile, compressive, flexural, shear, impact strengths and chloride permeability. The work demonstrates that the flow property inversely proposition with retempering time. Water absorption, sorptivity and chloride permeability for retempered concrete made by 20% substitute of cement by silica fume with additional 5% cement and water are lesser up to 60 min of retempering time. Compression, tension and flexural, shear, impact strengths for retempered concrete made by 20% substitute of cement by industrial waste silica fume with additional 5% cement and water are increased up to 60 min of retempering time, having strong microstructure than in the reference concrete. The prospect of substituting manufactured sand for natural sand and industrial by-products silica fume for cement has significant technical, economic, and environmental benefits, all of which are critical in today's construction climate also Instead of squandering bulk concrete, retempering using industrial waste and manufactured sand is advised.
first_indexed 2024-04-12T16:21:24Z
format Article
id doaj.art-d0bd6f14f56049d2b70885246f19f9e2
institution Directory Open Access Journal
issn 2772-3976
language English
last_indexed 2024-04-12T16:21:24Z
publishDate 2022-06-01
publisher Elsevier
record_format Article
series Cleaner Materials
spelling doaj.art-d0bd6f14f56049d2b70885246f19f9e22022-12-22T03:25:33ZengElsevierCleaner Materials2772-39762022-06-014100060Influence of retempering on properties of concrete made with manufactured sand and industrial wasteKiran M. Mane0Abhay M. Joshi1D.K. Kulkarni2K.B. Prakash3D. Y. Patil College of Engineering and Technology, Kolhapur 416006, Maharashtra, India; Corresponding author.D. Y. Patil College of Engineering and Technology, Kolhapur 416006, Maharashtra, IndiaDepartment of Civil Engineering, S.D.M. College of Engineering and Technology, Dharwad 580 002, Karanataka, IndiaGovt. Engineering College, Haveri, Devagiri 581 110, Karanataka, IndiaThe construction industry is currently dealing with a number of major issues. These include of shortage of river sand and large amount of energy required for manufacturing of cement produces free CO2 in air, accordingly use of manufactured sand and industrial waste in concrete increases. In construction of hilly topography long carrying of concrete is required, In outside location providing of concrete from inner mixing place, in construction of road, in lengthy tunneling work, manual transportation of concrete by labor, directly affect the flow property and concrete get stiff at the time of casting on real site work and in several conditions concrete get rejected by engineers. The paper discusses effects of replacing cement with 20% of industrial waste silica fumes and partially replacing natural sand with manufactured sand in the context of properties of retempered concrete like flow, water absorption, sorptivity, tensile, compressive, flexural, shear, impact strengths and chloride permeability. The work demonstrates that the flow property inversely proposition with retempering time. Water absorption, sorptivity and chloride permeability for retempered concrete made by 20% substitute of cement by silica fume with additional 5% cement and water are lesser up to 60 min of retempering time. Compression, tension and flexural, shear, impact strengths for retempered concrete made by 20% substitute of cement by industrial waste silica fume with additional 5% cement and water are increased up to 60 min of retempering time, having strong microstructure than in the reference concrete. The prospect of substituting manufactured sand for natural sand and industrial by-products silica fume for cement has significant technical, economic, and environmental benefits, all of which are critical in today's construction climate also Instead of squandering bulk concrete, retempering using industrial waste and manufactured sand is advised.http://www.sciencedirect.com/science/article/pii/S277239762200020XManufactured sandSilica fumeRetemperingWater absorptionSorptivityStrength
spellingShingle Kiran M. Mane
Abhay M. Joshi
D.K. Kulkarni
K.B. Prakash
Influence of retempering on properties of concrete made with manufactured sand and industrial waste
Cleaner Materials
Manufactured sand
Silica fume
Retempering
Water absorption
Sorptivity
Strength
title Influence of retempering on properties of concrete made with manufactured sand and industrial waste
title_full Influence of retempering on properties of concrete made with manufactured sand and industrial waste
title_fullStr Influence of retempering on properties of concrete made with manufactured sand and industrial waste
title_full_unstemmed Influence of retempering on properties of concrete made with manufactured sand and industrial waste
title_short Influence of retempering on properties of concrete made with manufactured sand and industrial waste
title_sort influence of retempering on properties of concrete made with manufactured sand and industrial waste
topic Manufactured sand
Silica fume
Retempering
Water absorption
Sorptivity
Strength
url http://www.sciencedirect.com/science/article/pii/S277239762200020X
work_keys_str_mv AT kiranmmane influenceofretemperingonpropertiesofconcretemadewithmanufacturedsandandindustrialwaste
AT abhaymjoshi influenceofretemperingonpropertiesofconcretemadewithmanufacturedsandandindustrialwaste
AT dkkulkarni influenceofretemperingonpropertiesofconcretemadewithmanufacturedsandandindustrialwaste
AT kbprakash influenceofretemperingonpropertiesofconcretemadewithmanufacturedsandandindustrialwaste