Influence of electrolysis parameters (concentration of silver in the electrolyte, current density, additives of surface active agents, a reversive current) on the granulometric composition and structure of silver powders is considered. Optimum conditions of the process are revealed.
Main Authors: | S. S. Zhuravleva, E. I. Pavlova, V. D. Ilyashevich, T. M. Buslaeva |
---|---|
Format: | Article |
Language: | Russian |
Published: |
MIREA - Russian Technological University
2011-06-01
|
Series: | Тонкие химические технологии |
Subjects: | |
Online Access: | https://www.finechem-mirea.ru/jour/article/view/841 |
Similar Items
-
Preparation and Investigation of Spherical Powder Made from Corrosion-Resistant 316L Steel with the Addition of 0.2% and 0.5% Ag
by: Mikhail A. Kaplan, et al.
Published: (2022-11-01) -
DEPOSITION OF YTTRIA STABILIZED ZIRCONIA THIN FILMS BY RADIO FREQUENCY MAGNETRON SPUTTERING FOR SOLID OXIDE FUEL CELL /
by: Siti Noryasmin Jaffar, 1992-, author, et al.
Published: (2017) -
DEPOSITION OF YTTRIA STABILIZED ZIRCONIA THIN FILMS BY RADIO FREQUENCY MAGNETRON SPUTTERING FOR SOLID OXIDE FUEL CELL /
by: Siti Noryasmin Jaffar, 1992-, author, et al.
Published: (2017) -
Study on the mechanism of forming silver nanoparticles on micron-scale flake silver powder
by: Lin Tang, et al.
Published: (2020-01-01) -
Influence of reducing agents and surfactants on size and shape of silver fine powder particles
by: Stevan P. Dimitrijević, et al.
Published: (2014-07-01)