Effect of local carbide formation behavior on repair weld liquation cracking susceptibility for long-term-serviced 247LC superalloy
This study assessed the liquation cracking temperature range (LCTR) for 247LC superalloy repair welds subjected to long-term and high-temperature exposure. To achieve this, the exposed specimens underwent simulations at 1273 K for 500, 1000, 3000, and 5000 h to replicate the long-term service condit...
Main Authors: | Hye-Eun Jeong, Seong-Moon Seo, Eun-Joon Chun |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2024-01-01
|
Series: | Journal of Materials Research and Technology |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2238785423030673 |
Similar Items
-
Suppression of liquation cracking susceptibility via pre-weld heat treatment for manufacturing of CM247LC superalloy turbine blade welds
by: Eun-Joon Chun, et al.
Published: (2021-11-01) -
Heat affected zone liquation cracking evaluation on FeMnAl alloys
by: Rafael Giorjao, et al.
Published: (2024-04-01) -
EFFECT OF TOOL ROTATION RATE IN FRICTION STIR SPOT WELDING ON LIQUATION CRACKING OF AZ91 ALLOY
by: F. Harati, et al.
Published: (2022-08-01) -
The Evolution of Cast Microstructures on the HAZ Liquation Cracking of Mar-M004 Weld
by: Yi-Hsin Cheng, et al.
Published: (2018-01-01) -
Analysis of liquation and solidification cracks in the electron beam welding of GTD-111 nickel-base superalloy joint
by: Morteza Taheri, et al.
Published: (2021-01-01)