Influence of self-healing property of Ultra-High Performance Concrete under aggressive environment

This paper investigates the evolution of self-healing properties of ultra-high performance concrete exposed to aggressive environments. Double edge wedge splitting UHPC specimens with 0.8% crystalline admixture and 1.5% steel fibre by volume have been first pre-cracked up to a average 0.30 mm crack...

Full description

Bibliographic Details
Main Authors: Xi Bin, Ferrara Liberato
Format: Article
Language:English
Published: EDP Sciences 2023-01-01
Series:MATEC Web of Conferences
Online Access:https://www.matec-conferences.org/articles/matecconf/pdf/2023/05/matecconf_smartincs2023_08003.pdf
_version_ 1797835267426484224
author Xi Bin
Ferrara Liberato
author_facet Xi Bin
Ferrara Liberato
author_sort Xi Bin
collection DOAJ
description This paper investigates the evolution of self-healing properties of ultra-high performance concrete exposed to aggressive environments. Double edge wedge splitting UHPC specimens with 0.8% crystalline admixture and 1.5% steel fibre by volume have been first pre-cracked up to a average 0.30 mm crack opening displacement (COD) obtained by two linear variable differential transformers attached to both sides of the sample surface. Then, the pre-cracked samples have been exposed to three different environments: tap water, salt water (a NaCl aqueous solution at 3.3% concentration) and geothermal water obtained from a geothermal power plant. After one month exposure, samples were carried out re-crack to know the self-healing properties. The results from ultrasonic pulse velocity tests (UPV) reveal that the samples exposed to tap water exhibit the highest rate of recovery along the exposure time, while those exposed to geothermal water show the lowest. The calculated indexes of cracking self-healing (ICS) show a 73.8% closure in tap water, 58.4% in salt water 43.9% in geothermal water. Additionally, the index of damage recovery, evaluated from UPV frequencies as well as from the stress vs. COD curves of pre-cracking and post-healing re-cracking tests on specimens, and the equivalent tensile stress also indicate a higher level of healing capable of inducing a significant recovery of mechanical properties.
first_indexed 2024-04-09T14:51:27Z
format Article
id doaj.art-dfc1561b545c452c83df69e4db440a06
institution Directory Open Access Journal
issn 2261-236X
language English
last_indexed 2024-04-09T14:51:27Z
publishDate 2023-01-01
publisher EDP Sciences
record_format Article
series MATEC Web of Conferences
spelling doaj.art-dfc1561b545c452c83df69e4db440a062023-05-02T09:34:12ZengEDP SciencesMATEC Web of Conferences2261-236X2023-01-013780800310.1051/matecconf/202337808003matecconf_smartincs2023_08003Influence of self-healing property of Ultra-High Performance Concrete under aggressive environmentXi Bin0Ferrara Liberato1Department of Civil and Environmental Engineering, Politecnico di MilanoDepartment of Civil and Environmental Engineering, Politecnico di MilanoThis paper investigates the evolution of self-healing properties of ultra-high performance concrete exposed to aggressive environments. Double edge wedge splitting UHPC specimens with 0.8% crystalline admixture and 1.5% steel fibre by volume have been first pre-cracked up to a average 0.30 mm crack opening displacement (COD) obtained by two linear variable differential transformers attached to both sides of the sample surface. Then, the pre-cracked samples have been exposed to three different environments: tap water, salt water (a NaCl aqueous solution at 3.3% concentration) and geothermal water obtained from a geothermal power plant. After one month exposure, samples were carried out re-crack to know the self-healing properties. The results from ultrasonic pulse velocity tests (UPV) reveal that the samples exposed to tap water exhibit the highest rate of recovery along the exposure time, while those exposed to geothermal water show the lowest. The calculated indexes of cracking self-healing (ICS) show a 73.8% closure in tap water, 58.4% in salt water 43.9% in geothermal water. Additionally, the index of damage recovery, evaluated from UPV frequencies as well as from the stress vs. COD curves of pre-cracking and post-healing re-cracking tests on specimens, and the equivalent tensile stress also indicate a higher level of healing capable of inducing a significant recovery of mechanical properties.https://www.matec-conferences.org/articles/matecconf/pdf/2023/05/matecconf_smartincs2023_08003.pdf
spellingShingle Xi Bin
Ferrara Liberato
Influence of self-healing property of Ultra-High Performance Concrete under aggressive environment
MATEC Web of Conferences
title Influence of self-healing property of Ultra-High Performance Concrete under aggressive environment
title_full Influence of self-healing property of Ultra-High Performance Concrete under aggressive environment
title_fullStr Influence of self-healing property of Ultra-High Performance Concrete under aggressive environment
title_full_unstemmed Influence of self-healing property of Ultra-High Performance Concrete under aggressive environment
title_short Influence of self-healing property of Ultra-High Performance Concrete under aggressive environment
title_sort influence of self healing property of ultra high performance concrete under aggressive environment
url https://www.matec-conferences.org/articles/matecconf/pdf/2023/05/matecconf_smartincs2023_08003.pdf
work_keys_str_mv AT xibin influenceofselfhealingpropertyofultrahighperformanceconcreteunderaggressiveenvironment
AT ferraraliberato influenceofselfhealingpropertyofultrahighperformanceconcreteunderaggressiveenvironment