The influence of the heat treatment on delta ferrite transformation in austenitic stainless steel welds
Shielded metal arc (SMAW) welded specimens using austenitic consumable materials with different amount of delta-ferrite are annealed in range 650-750 °C through 2-10 hours. Factorial plan 3<sup>3</sup> with influenced factors regression analyze of measured delta-ferrite values is used. T...
Main Authors: | B. Mateša, I. Samardžić, M. Dunđer |
---|---|
Format: | Article |
Language: | English |
Published: |
Croatian Metallurgical Society
2012-04-01
|
Series: | Metalurgija |
Subjects: | |
Online Access: | http://hrcak.srce.hr/file/111123 |
Similar Items
-
Nondestructive Microstructural Characterization of Austenitic-Ferritic Stainless Steel Welded Joints by Double Loop Electrochemical Polarization Reactivation Portable Test
by: Brígida Bastos de Almeida, et al.
Published: (2022-01-01) -
Transformation of the δ-Ferrite in SS2343 Austenitic Stainless Steel upon Annealing at 1050 °C, 1150 °C and 1250 °C
by: Boštjan Arh, et al.
Published: (2021-06-01) -
Delta ferrite formation and evolution during slab processing from an 80-ton industrial heat of AISI 304 austenitic stainless steel
by: Flávia Andressa Moreira dos Santos, et al.
Published: (2023-01-01) -
Influence of delta ferrite on corrosion susceptibility of AISI 304 austenitic stainless steel
by: Lawrence O. Osoba, et al.
Published: (2016-12-01) -
Corrosion of an austenite and ferrite stainless steel weld
by: BRANIMIR N. GRGUR, et al.
Published: (2011-07-01)