Effect of Residual Deformation Energy and Critical Heating Rate on Cubic Texture and Grain Growth Behavior of Severely Deformed Aluminum Foil
To clarify the microstructure, grain size, and recrystallization behavior during different annealing processes with controlled heating rates, the aim of this study was to investigate the effect of residual deformation energy after cold rolling and critical heating rate on cubic texture components, a...
Main Authors: | Yunlei Wang, Liping Ren, Qi Liu, Yu Cao, Guangjie Huang |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2022-02-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/15/4/1395 |
Similar Items
-
Grain Rotation in Plastic Deformation
by: Bin Chen, et al.
Published: (2019-07-01) -
Welding deformation and residual stress prevention /
by: Ueda, Yukio, et al.
Published: (c201) -
Polycrystal Simulation of Texture-Induced Grain Coarsening during Severe Plastic Deformation
by: Chi Zhang, et al.
Published: (2020-12-01) -
The effect of grain size on deformation modes and deformation heterogeneity in a rolled Mg–Zn–Ca alloy
by: Haoge Shou, et al.
Published: (2023-01-01) -
Deformation evolution depending on grain boundary type and hydrogen concentration in nickel investigated by molecular dynamics simulation
by: Yuanyuan Zheng, et al.
Published: (2022-01-01)