Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer Crowns
Introduction: Marginal discrepancy severely affects the long term success of All ceramic complete veneer crowns. The precise role of resin luting agents influencing this phenomenon needs to be explored further. Aim: To estimate and compare the marginal discrepancy in CAD/CAM processed All ceram...
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
JCDR Research and Publications Private Limited
2016-12-01
|
Series: | Journal of Clinical and Diagnostic Research |
Subjects: | |
Online Access: | https://jcdr.net/articles/PDF/9028/21447_CE[NE]_F(Sh)_PF1(NEAK)_PFA(AK)_PF2(EKAK).pdf |
_version_ | 1818363837360898048 |
---|---|
author | Dhanraj Ganapathy Anusha Sathyamoorthy Hemalatha Ranganathan Karthikeyan Murthykumar |
author_facet | Dhanraj Ganapathy Anusha Sathyamoorthy Hemalatha Ranganathan Karthikeyan Murthykumar |
author_sort | Dhanraj Ganapathy |
collection | DOAJ |
description | Introduction: Marginal discrepancy severely affects the long
term success of All ceramic complete veneer crowns. The
precise role of resin luting agents influencing this phenomenon
needs to be explored further.
Aim: To estimate and compare the marginal discrepancy in
CAD/CAM processed All ceramic complete veneer crowns prior
and following luting with resin bonded luting agents.
Materials and Methods: Extracted human maxillary first
premolars were randomly allocated into four groups of 27
samples each Viz., Group I-Resin Modified Glass Ionomer
Cement (GIC) (RelyX), Group II-Bis-GMA based dual cure resin
cement (Variolink II), Group III-PMMA based resin cement
(Superbond), Group IV- Urethane Dimethacrylate resin cement
(Calibra). Following tooth preparation, CAD/CAM All ceramic
complete veneer crowns were fabricated and sectioned and
marginal discrepancy was evaluated using a scanning electron
microscope (TESCAN, Magnification power-1,00,000x) prior
and after luting with the experimental resin cements.
Results: The vertical and horizontal discrepancy before and after
cementation with Group I [270.08±103.10µm, 165.3±53.00µm
and 270.86±102.70µm, 166.62±54.96µm respectively]; Group
II [254.21±79.20µm, 117.75±24.29µm and 234.81±79µm,
116.89±18.22µm respectively]; Group III [272.47±86.25µm,
142.08±50.83µm and 251.82±62.69µm, 136.07±44.95µm
respectively]; Group IV were [260.28±64.81µm, 116.98±17.71µm
and 233.08±69.44µm, 116.58±21.13µm respectively]. ANOVA
inferred a statistically significant difference between the four
test specimen with regards to vertical and horizontal marginal
discrepancy after cementation (F=9.092, p<0.001), (F=10.97,
p<0.001). Tukey HSD Post-hoc test observed significant
differences in vertical and horizontal marginal discrepancies
between the resin modified glass ionomer and resin cements
(p<0.05).
Conclusion: Resin cements exhibited a greater reduction in
the marginal discrepancy than the resin modified glass ionomer
following luting in All ceramic complete veneer crowns. Hence
resin cements are more preferable to GIC for luting All ceramic
complete veneer crowns. |
first_indexed | 2024-12-13T21:54:49Z |
format | Article |
id | doaj.art-e3e2baba56194aa29b0a1986d1d24af2 |
institution | Directory Open Access Journal |
issn | 2249-782X 0973-709X |
language | English |
last_indexed | 2024-12-13T21:54:49Z |
publishDate | 2016-12-01 |
publisher | JCDR Research and Publications Private Limited |
record_format | Article |
series | Journal of Clinical and Diagnostic Research |
spelling | doaj.art-e3e2baba56194aa29b0a1986d1d24af22022-12-21T23:30:10ZengJCDR Research and Publications Private LimitedJournal of Clinical and Diagnostic Research2249-782X0973-709X2016-12-011012ZC67ZC7010.7860/JCDR/2016/21447.9028Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer CrownsDhanraj Ganapathy0Anusha Sathyamoorthy1Hemalatha Ranganathan2Karthikeyan Murthykumar3Professor and HOD, Department of Prosthodontics, Saveetha Dental College, Chennai, Tamil Nadu, India.Postgraduate Student, Department of Prosthodontics, Saveetha Dental College, Chennai, Tamil Nadu, India.Postgraduate Student, Department of Prosthodontics, Saveetha Dental College, Chennai, Tamil Nadu, India.Intern, Department of Prosthodontics, Saveetha Dental College, Chennai, Tamil Nadu, India.Introduction: Marginal discrepancy severely affects the long term success of All ceramic complete veneer crowns. The precise role of resin luting agents influencing this phenomenon needs to be explored further. Aim: To estimate and compare the marginal discrepancy in CAD/CAM processed All ceramic complete veneer crowns prior and following luting with resin bonded luting agents. Materials and Methods: Extracted human maxillary first premolars were randomly allocated into four groups of 27 samples each Viz., Group I-Resin Modified Glass Ionomer Cement (GIC) (RelyX), Group II-Bis-GMA based dual cure resin cement (Variolink II), Group III-PMMA based resin cement (Superbond), Group IV- Urethane Dimethacrylate resin cement (Calibra). Following tooth preparation, CAD/CAM All ceramic complete veneer crowns were fabricated and sectioned and marginal discrepancy was evaluated using a scanning electron microscope (TESCAN, Magnification power-1,00,000x) prior and after luting with the experimental resin cements. Results: The vertical and horizontal discrepancy before and after cementation with Group I [270.08±103.10µm, 165.3±53.00µm and 270.86±102.70µm, 166.62±54.96µm respectively]; Group II [254.21±79.20µm, 117.75±24.29µm and 234.81±79µm, 116.89±18.22µm respectively]; Group III [272.47±86.25µm, 142.08±50.83µm and 251.82±62.69µm, 136.07±44.95µm respectively]; Group IV were [260.28±64.81µm, 116.98±17.71µm and 233.08±69.44µm, 116.58±21.13µm respectively]. ANOVA inferred a statistically significant difference between the four test specimen with regards to vertical and horizontal marginal discrepancy after cementation (F=9.092, p<0.001), (F=10.97, p<0.001). Tukey HSD Post-hoc test observed significant differences in vertical and horizontal marginal discrepancies between the resin modified glass ionomer and resin cements (p<0.05). Conclusion: Resin cements exhibited a greater reduction in the marginal discrepancy than the resin modified glass ionomer following luting in All ceramic complete veneer crowns. Hence resin cements are more preferable to GIC for luting All ceramic complete veneer crowns.https://jcdr.net/articles/PDF/9028/21447_CE[NE]_F(Sh)_PF1(NEAK)_PFA(AK)_PF2(EKAK).pdfbis-gma resincad/cam crownsglass ionomer cementmarginal adaptationurethane dimethacrylate resin |
spellingShingle | Dhanraj Ganapathy Anusha Sathyamoorthy Hemalatha Ranganathan Karthikeyan Murthykumar Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer Crowns Journal of Clinical and Diagnostic Research bis-gma resin cad/cam crowns glass ionomer cement marginal adaptation urethane dimethacrylate resin |
title | Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer Crowns |
title_full | Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer Crowns |
title_fullStr | Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer Crowns |
title_full_unstemmed | Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer Crowns |
title_short | Effect of Resin Bonded Luting Agents Influencing Marginal Discrepancy in All Ceramic Complete Veneer Crowns |
title_sort | effect of resin bonded luting agents influencing marginal discrepancy in all ceramic complete veneer crowns |
topic | bis-gma resin cad/cam crowns glass ionomer cement marginal adaptation urethane dimethacrylate resin |
url | https://jcdr.net/articles/PDF/9028/21447_CE[NE]_F(Sh)_PF1(NEAK)_PFA(AK)_PF2(EKAK).pdf |
work_keys_str_mv | AT dhanrajganapathy effectofresinbondedlutingagentsinfluencingmarginaldiscrepancyinallceramiccompleteveneercrowns AT anushasathyamoorthy effectofresinbondedlutingagentsinfluencingmarginaldiscrepancyinallceramiccompleteveneercrowns AT hemalatharanganathan effectofresinbondedlutingagentsinfluencingmarginaldiscrepancyinallceramiccompleteveneercrowns AT karthikeyanmurthykumar effectofresinbondedlutingagentsinfluencingmarginaldiscrepancyinallceramiccompleteveneercrowns |