The prediction of evaluation a U- and V-shaped cracks on the surface and subsurface of a continuously cast steel slab, is investigated during hot rolling. The numerical simulation is carried out by means of FE-code DEFORM 3D. Therefore, an algorithmic decision tree was developed by the C 4.5 program...
Main Authors: | Vlado Martin, Bidulský Róbert, Gulová Lucia, Machová Kristína, Bidulská Jana, Valíček Ján, Sas Ján |
---|---|
Format: | Article |
Language: | English |
Published: |
De Gruyter
2011-04-01
|
Series: | High Temperature Materials and Processes |
Subjects: | |
Online Access: | https://doi.org/10.1515/htmp.2011.014 |
Similar Items
-
Analysis of Internal Cracks in Continuous Casting Slabs with Soft Reduction
by: Wang Bo, et al.
Published: (2016-03-01) -
Improving Slab Quality Through Control of Cooling Parameters in Continuous Casting Plants
by: Marian BORDEI, et al.
Published: (2014-12-01) -
Experimental study on evolution of oxidation behavior on high-temperature continuous casting slab surface
by: Siyuan Zhang, et al.
Published: (2021-03-01) -
A Prediction Model for Internal Cracks during Slab Continuous Casting
by: Yiwen Kong, et al.
Published: (2019-05-01) -
Fluid Flow in Continuous Casting Mold for Ultra-Wide Slab
by: Gang Li, et al.
Published: (2023-01-01)