Extraction of Gold and Copper from Flotation Tailings Using Glycine-Ammonia Solutions in the Presence of Permanganate

This study presents the novel idea of a cyanide-free leaching method, i.e., glycine-ammonia leaching in the presence of permanganate, to treat a low-grade and copper-bearing gold tailing. Ammonia played a key role as a pH modifier, lixiviant and potential catalyst (as cupric ammine) in this study. R...

Full description

Bibliographic Details
Main Authors: Huan Li, Elsayed Oraby, Jacques Eksteen, Tanmay Mali
Format: Article
Language:English
Published: MDPI AG 2022-05-01
Series:Minerals
Subjects:
Online Access:https://www.mdpi.com/2075-163X/12/5/612
Description
Summary:This study presents the novel idea of a cyanide-free leaching method, i.e., glycine-ammonia leaching in the presence of permanganate, to treat a low-grade and copper-bearing gold tailing. Ammonia played a key role as a pH modifier, lixiviant and potential catalyst (as cupric ammine) in this study. Replacing ammonia with other pH modifiers (i.e., sodium hydroxide or lime) made the extractions infeasibly low (<30%). The increased additions of glycine (23–93 kg/t), ammonia (30–157 kg/t) and permanganate (5–20 kg/t) enhanced gold and copper extractions considerably. Increasing the solids content from 20 to 40% did not make any obvious changes to copper extraction. However, gold leaching kinetics was slightly better at lower solids content. It was indicated that the staged addition of permanganate was unnecessary under the leaching conditions. Recovery of gold by CIL was shown to be feasible, and it improved gold extraction by 15%, but no effect was observed for copper extraction. Percentages of 76.5% gold and 64.5% copper were extracted in 48 h at 20 g/L glycine, 10 kg/t permanganate, 20 g/L carbon, pH 10.5 and 30% solids. Higher extractions could be potentially achieved by further optimization, such as by increasing permanganate addition, extending leaching time and ultra-fine grinding.