Acoustic and optical phonons in metallic diamond

The dispersion of acoustic and optical phonons in highly boron-doped diamond has been measured by inelastic X-ray scattering at an energy resolution of 6.4 meV. The sample is doped in the metallic regime and shows superconductivity below 4.2 K (midpoint). The data are compared to pure and nitrogen-d...

وصف كامل

التفاصيل البيبلوغرافية
المؤلف الرئيسي: M. Hoesch, T. Fukuda, T. Takenouchi, J.P. Sutter, S. Tsutsui, A.Q.R. Baron, M. Nagao, Y. Takano, H. Kawarada and J. Mizuki
التنسيق: مقال
اللغة:English
منشور في: Taylor & Francis Group 2006-01-01
سلاسل:Science and Technology of Advanced Materials
الوصول للمادة أونلاين:http://www.iop.org/EJ/abstract/-search=58672466.19/1468-6996/7/S1/A08