Deformation behaviour of laser-welded tube blank of TA15 Ti-alloy for gas forming at elevated temperature
Deformation behaviour of laser-welded tube blank of TA15 Ti-alloy at elevated temperature was investigated by both hot tensile tests and high pressure gas forming(HPGF). The hot tensile tests were carried out with four different specimens at 800 ∘C with an initial strain rate of 1.00×10−2 s−1 and HP...
Main Authors: | Wang Kehuan, Liu Gang, Yuan Shijian |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2015-01-01
|
Series: | MATEC Web of Conferences |
Online Access: | http://dx.doi.org/10.1051/matecconf/20152106005 |
Similar Items
-
Forming analysis of tailor welded blank /
by: 381525 Mahfodzah Md. Padzi, et al.
Published: (2007) -
Forming analysis of tailor welded blank /
by: 420719 Mohamed Shariff Razuli, et al.
Published: (2007) -
Fatigue behaviour of aluminium 6061 in tailor welded blank
by: Wan Iryana, Wan Md Nor
Published: (2013) -
Forming analysis of tailor welded blank [electronic resource] /
by: 381525 Mahfodzah Md. Padzi
Published: (2007) -
Forming analysis of tailor welded blank [electronic resource] /
by: 420719 Mohamed Shariff Razuli
Published: (2007)