Sintering and Properties of W-25% Re Composition for Sermet Fuel Production by Spark Plasma Method
In this study, the sintering of tungsten metal powders of 99.99% purity and 7.8 µm for cermet production by Spark Plasma Sintering (SPS) method at temperatures between 1300°C and 1700°C for 5 minutes, 10 minutes, 20 minutes and 30 minutes was investigated. The relative densities of the sintered tung...
Main Author: | Hüseyin ADANIR |
---|---|
Format: | Article |
Language: | English |
Published: |
Gazi University
2019-12-01
|
Series: | Gazi Üniversitesi Fen Bilimleri Dergisi |
Subjects: | |
Online Access: | https://dergipark.org.tr/tr/download/article-file/878469 |
Similar Items
-
Effect of Rhenium addition on tungsten heavy alloys processed through spark plasma sintering
by: B.S. Lakshmi Prasad, et al.
Published: (2021-09-01) -
Ultrafine-Grained Tungsten Heavy Alloy Prepared by High-Pressure Spark Plasma Sintering
by: Shuaihao Zhang, et al.
Published: (2022-09-01) -
Activated sintering effect of Fe element on tungsten via spark plasma sintering
by: Shuai Chen, et al.
Published: (2022-09-01) -
Spark Plasma Sintering of WC-Based 10wt%Co Hard Alloy: A Study of Sintering Kinetics and Solid-Phase Processes
by: Anastasia A. Buravleva, et al.
Published: (2022-01-01) -
Powder Metallurgical Processing and Characterization of Molybdenum Addition to Tungsten Heavy Alloys by Spark Plasma Sintering
by: A. Raja Annamalai, et al.
Published: (2021-10-01)