The Failure Mechanism of the 316 SS Heat Exchanger Tube in the Geothermal Water Environment
In this work, the intrinsic reason for the premature failure of a 316 stainless steel heat exchanger tube in geothermal water environment is disclosed. The chemical composition of the tube was tested, and the microstructure was examined for material inspection. Fracture morphology and secondary crac...
Main Authors: | Jike Yang, Chan Li, Yue Pan, Hui Huang |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2022-11-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/15/22/8103 |
Similar Items
-
Corrosion of 316L Stainless Steel Tubes of High Pressure Heat Exchanger
by: Mohammed Hussain Ahmed
Published: (2005-08-01) -
Analysis of Corrosion of Hastelloy-N, Alloy X750, SS316 and SS304 in Molten Salt High-Temperature Environment
by: Ketan Kumar Sandhi, et al.
Published: (2021-01-01) -
Stress corrosion cracking of 316LN stainless steel with orthogonal scratches
by: Zhiheng Xiong, et al.
Published: (2023-05-01) -
A Review of Electrochemical Corrosion on Stainless Steel 316
by: K. BARANIDHARAN, et al.
Published: (2020-12-01) -
Comprehensive review of various corrosion behaviours on 316 stainless steel
by: Baranidharan K, et al.
Published: (2021-01-01)