Flow Behavior Characteristics and Processing Map of Fe-6.5wt. %Si Alloys during Hot Compression
The flow behavior of Fe-6.5wt. %Si alloys during hot compression was investigated at temperatures 650–950 °C and strain rates 0.01–10 s−1. The results showed that the flow stress depended distinctly on the deformation temperatures and strain rates. The flow stress and work hardening rate increased w...