Flow Behavior Characteristics and Processing Map of Fe-6.5wt. %Si Alloys during Hot Compression
The flow behavior of Fe-6.5wt. %Si alloys during hot compression was investigated at temperatures 650–950 °C and strain rates 0.01–10 s−1. The results showed that the flow stress depended distinctly on the deformation temperatures and strain rates. The flow stress and work hardening rate increased w...
Main Authors: | Shibo Wen, Chaoyu Han, Bao Zhang, Yongfeng Liang, Feng Ye, Junpin Lin |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2018-03-01
|
Series: | Metals |
Subjects: | |
Online Access: | http://www.mdpi.com/2075-4701/8/3/186 |
Similar Items
-
Fabrication Technology and Material Characterization of Hot Rolled Cylindrical Fe-6.5 wt. % Si Bars
by: Shibo Wen, et al.
Published: (2018-05-01) -
Microstructure, Texture Evolution and Magnetic Properties of Fe-6.5 wt. % Si and Fe-6.5 wt. % Si-0.5 wt. % Cu Alloys during Rolling and Annealing Treatment
by: Zhaoyang Cheng, et al.
Published: (2018-02-01) -
Serrated Flow Behavior of Hot-Rolled Fe-6.5wt.%Si Sheet with Layered Structure
by: Xiangju Shi, et al.
Published: (2019-09-01) -
AC Iron Loss Prediction and Magnetic Properties of Fe-6.5 wt. % Si Ribbons Prepared by Melt-Spinning
by: Shuai Wang, et al.
Published: (2018-04-01) -
Effects of yttrium on the microstructure, texture, and magnetic properties of non-oriented 6.5 wt% Si steel sheets by a rolling process
by: Jing Qin, et al.
Published: (2021-01-01)