CORROSION RESISTANCE OF SELF-COMPACTING CONCRETE CONTAINING CALCIUM STEARATE

This study aims to determine the corrosion resistance of self-compacting concrete (SCC) combined with calcium stearate (CS), Ca(C18H35O2)2. The concrete qualities tested are 20, 30, and 40 MPa. The CS dose used ranges from 0 to 2.85% of the cement weight. Two types of testing were performed in this...