Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings

The Secondary Electron Emission (SEE) from the Plasma Facing Components, (PFCs) affects the plasma sheath and edge structure of magnetically confined toroidal plasmas with effects on the Scrappe Off Layer (SOL), heat transport and incident plasma heat flux to the divertor targets. It is also behind...

Full description

Bibliographic Details
Main Authors: A. de Castro, E. Oyarzábal, F.L. Tabarés
Format: Article
Language:English
Published: Elsevier 2023-03-01
Series:Nuclear Materials and Energy
Subjects:
Online Access:http://www.sciencedirect.com/science/article/pii/S2352179123000273
_version_ 1811154370080800768
author A. de Castro
E. Oyarzábal
F.L. Tabarés
author_facet A. de Castro
E. Oyarzábal
F.L. Tabarés
author_sort A. de Castro
collection DOAJ
description The Secondary Electron Emission (SEE) from the Plasma Facing Components, (PFCs) affects the plasma sheath and edge structure of magnetically confined toroidal plasmas with effects on the Scrappe Off Layer (SOL), heat transport and incident plasma heat flux to the divertor targets. It is also behind the performance degradation in aerospace devices as Hall thrusters. In future reactor prototypes using tungsten (W) components, much more demanding and longer term conditions for the exposed PFCs are expected. These scenarios will exacerbate the material degradation of the exposed surfaces that will change its morphology, thus modifying its plasma material interaction behavior. In such scenario, specific studies on the influence of the microstructure in the tungsten SEE yields become necessary. In these laboratory experiments, the SEE emission of different microstructured tungsten coatings exposed to helium Glow Discharge (GD) plasmas has been analyzed by using a previously developed laboratory technique. It enables the characterization of the I-V characteristics of the biased sample and, at the same time, the acquisition of the electron incident flux by using a gridded probe adjacent to the exposed sample. Different microstructured W coated samples differing in coating thickness (2500 nm and 500 nm) and primal substrate surface finishing (translated in final differences within the W coating topologies) were analyzed, also including cold rolled tungsten and original stainless steel (SS) substrate (material in which the microstructured tungsten film was deposited) as benchmarks for comparison. The overall results have shown that the presence of a 2500 nm thick microstructured W coating decreases the SEE yield of tungsten (cold rolled) up to a factor 40 % at electron mean energies of 100–175 eV. Conversely, 500 nm coatings did not reduce the SEE yield even showing an increase at 25–100 eV. The final increase/decrease in the obtained SEE yields seems to be more influenced by the microstructured coating thickness (where the role of intrinsic differences in oxygen content of the surfaces is discussed) rather than other questions possibly derived by the differences in surface topology (ordering, directionality and/or roughness of the microstructure features).
first_indexed 2024-04-10T04:15:35Z
format Article
id doaj.art-f7653d5702d84e40b2aa6b4dbdacd79c
institution Directory Open Access Journal
issn 2352-1791
language English
last_indexed 2024-04-10T04:15:35Z
publishDate 2023-03-01
publisher Elsevier
record_format Article
series Nuclear Materials and Energy
spelling doaj.art-f7653d5702d84e40b2aa6b4dbdacd79c2023-03-12T04:21:34ZengElsevierNuclear Materials and Energy2352-17912023-03-0134101388Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatingsA. de Castro0E. Oyarzábal1F.L. Tabarés2Corresponding author.; Laboratorio Nacional de Fusión, Av. Complutense, 40, 28040 Madrid, SpainLaboratorio Nacional de Fusión, Av. Complutense, 40, 28040 Madrid, SpainLaboratorio Nacional de Fusión, Av. Complutense, 40, 28040 Madrid, SpainThe Secondary Electron Emission (SEE) from the Plasma Facing Components, (PFCs) affects the plasma sheath and edge structure of magnetically confined toroidal plasmas with effects on the Scrappe Off Layer (SOL), heat transport and incident plasma heat flux to the divertor targets. It is also behind the performance degradation in aerospace devices as Hall thrusters. In future reactor prototypes using tungsten (W) components, much more demanding and longer term conditions for the exposed PFCs are expected. These scenarios will exacerbate the material degradation of the exposed surfaces that will change its morphology, thus modifying its plasma material interaction behavior. In such scenario, specific studies on the influence of the microstructure in the tungsten SEE yields become necessary. In these laboratory experiments, the SEE emission of different microstructured tungsten coatings exposed to helium Glow Discharge (GD) plasmas has been analyzed by using a previously developed laboratory technique. It enables the characterization of the I-V characteristics of the biased sample and, at the same time, the acquisition of the electron incident flux by using a gridded probe adjacent to the exposed sample. Different microstructured W coated samples differing in coating thickness (2500 nm and 500 nm) and primal substrate surface finishing (translated in final differences within the W coating topologies) were analyzed, also including cold rolled tungsten and original stainless steel (SS) substrate (material in which the microstructured tungsten film was deposited) as benchmarks for comparison. The overall results have shown that the presence of a 2500 nm thick microstructured W coating decreases the SEE yield of tungsten (cold rolled) up to a factor 40 % at electron mean energies of 100–175 eV. Conversely, 500 nm coatings did not reduce the SEE yield even showing an increase at 25–100 eV. The final increase/decrease in the obtained SEE yields seems to be more influenced by the microstructured coating thickness (where the role of intrinsic differences in oxygen content of the surfaces is discussed) rather than other questions possibly derived by the differences in surface topology (ordering, directionality and/or roughness of the microstructure features).http://www.sciencedirect.com/science/article/pii/S2352179123000273TungstenSecondary electron emissionSurface microstructure
spellingShingle A. de Castro
E. Oyarzábal
F.L. Tabarés
Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings
Nuclear Materials and Energy
Tungsten
Secondary electron emission
Surface microstructure
title Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings
title_full Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings
title_fullStr Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings
title_full_unstemmed Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings
title_short Cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings
title_sort cold plasma studies on the influence of surface microstructured thickness in the secondary electron emission from tungsten coatings
topic Tungsten
Secondary electron emission
Surface microstructure
url http://www.sciencedirect.com/science/article/pii/S2352179123000273
work_keys_str_mv AT adecastro coldplasmastudiesontheinfluenceofsurfacemicrostructuredthicknessinthesecondaryelectronemissionfromtungstencoatings
AT eoyarzabal coldplasmastudiesontheinfluenceofsurfacemicrostructuredthicknessinthesecondaryelectronemissionfromtungstencoatings
AT fltabares coldplasmastudiesontheinfluenceofsurfacemicrostructuredthicknessinthesecondaryelectronemissionfromtungstencoatings