Evaporated Alkali Carbonate Effect on an Aluminum Diffusion Coated 253MA Vessel after 4000 h Discontinuous Operation—Lessons Learned
A vessel of a laboratory setup for hosting molten alkali carbonate immersion experiments was recently decommissioned after about 4000 h discontinuous operation at 800 °C. In this article, we want to describe the long-term damage of the vessel caused by evaporated alkali carbonate species in a carbon...
Main Authors: | Esraa Hamdy, Angelina Wagné, Christine Geers |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2022-04-01
|
Series: | Energies |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1073/15/9/3241 |
Similar Items
Similar Items
-
Effect of Grain Size on Mechanical and Creep Rupture Properties of 253 MA Austenitic Stainless Steel
by: Mochammad Syaiful Anwar, et al.
Published: (2022-05-01) -
O rizoma hipertextual no romance digital 253, de Geoff Ryman
by: Alice Garcia Silveira, et al.
Published: (2020-01-01) -
Publius Ovidius Naso: Pazifaa (Ars amatoria 1, 253-350)
by: Barbara Šega Čeh
Published: (2001-07-01) -
Integrated profiling identifies DXS253E as a potential prognostic marker in colorectal cancer
by: Pu Xing, et al.
Published: (2024-06-01) -
Investigation on AISI 253 Stainless Steel by Gas Nitriding Process for Sustainable Applications
by: Ramyasree K., et al.
Published: (2024-01-01)