A Modified Constitutive Model for the Description of the Flow Behavior of the Ti-10V-2Fe-3Al Alloy during Hot Plastic Deformation
The hot deformation behavior of the aerospace Ti-10-2-3 alloy was investigated by isothermal compression tests at temperatures of 740 to 820 °C and strain rates of 0.0005 to 10 s<sup>−1</sup>. The results show that the studied alloy is extremely sensitive to deformatio...
Main Authors: | Fukang Wang, Jingyuan Shen, Yong Zhang, Yongquan Ning |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2019-07-01
|
Series: | Metals |
Subjects: | |
Online Access: | https://www.mdpi.com/2075-4701/9/8/844 |
Similar Items
-
Hot deformation behaviours and spheroidization mechanisms of Ti-5322 alloy during hot compression
by: Andong Wang, et al.
Published: (2021-01-01) -
Mechanical behaviour and microstructural evolution of Ti–6Al–1Mo–1V–2Zr–2Cr–1Fe alloy subjected to hot compression deformation
by: Youchuan Mao, et al.
Published: (2023-11-01) -
Hot Deformation and Constitutive Modeling of TC21 Titanium Alloy
by: Sheng-Xian Yi, et al.
Published: (2022-03-01) -
Hot deformation behavior and constitutive equation of TB8 titanium alloy with a lamellar structure of α phase
by: ZHOU Ya-li, et al.
Published: (2021-01-01) -
Constitutive equation and microstructure evolution of TiAl alloy during hot deformation
by: Shiwei Tian, et al.
Published: (2023-01-01)