Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061

Friction Stir Welding (FSW) is a solid-state welding method that has diffusion and different metal structures can blend well. Friction stir welding (FSW) has a weakness, one of which is the lack of flexibility the welding process is only carried out on one side of the plate being welded, so it is no...

Full description

Bibliographic Details
Main Authors: Danang Priyasudana, Simonne Andrean Crisdion, Poppy Puspitasari, Triyono, Jamasri, Andoko, Diki Dwi Pramono
Format: Article
Language:English
Published: Elsevier 2023-02-01
Series:Heliyon
Subjects:
Online Access:http://www.sciencedirect.com/science/article/pii/S240584402300573X
_version_ 1811161795134488576
author Danang Priyasudana
Simonne Andrean Crisdion
Poppy Puspitasari
Triyono
Jamasri
Andoko
Diki Dwi Pramono
author_facet Danang Priyasudana
Simonne Andrean Crisdion
Poppy Puspitasari
Triyono
Jamasri
Andoko
Diki Dwi Pramono
author_sort Danang Priyasudana
collection DOAJ
description Friction Stir Welding (FSW) is a solid-state welding method that has diffusion and different metal structures can blend well. Friction stir welding (FSW) has a weakness, one of which is the lack of flexibility the welding process is only carried out on one side of the plate being welded, so it is not applied on thick materials. Double side friction stir welding is a double working process in which the plate to be welded is subjected to friction from two tools on opposite sides. In the DS-FSW welding process, the dimensions and geometry of the tool and pin greatly affect the quality of the joint. This study to determine the mechanical properties and corrosion rate of Double side friction stir welding aluminum 6061 with variation rotation speed and axis of top and bottom tools. The results of this radiographic test can be seen that specimen 4 welded with variations in speed and tool position has defects in the form of incomplete fusion (IF). The results of microstructural observations showed that the heat caused by the welding process resulted in recrystallization in the form of fine grains in the stirring area and there was no phase change. The highest hardness value in the welding area is specimen B. The largest bending value at the 1G welding positions is specimen D, which is 41.86 MPa with a strain value of 13.23%, while the smallest value at the 4G welding position is specimen A, which is 38.18 MPa with a strain value of 5.03%. The fracture and crack surfaces showed that crack initiation, propagation and material stirring failure occurred in all test specimens, even though the impact test specimen was cut in a small area of Incomplete Fusion, but the test results showed that there was still a surface of the parent metal that had not been stirred. The corrosion test method uses three electrode cells with corrosion media as a substitute for seawater with a salinity of 3.5% NaCl, result of corrosion test is specimen B at the 1G welding position has the highest corrosion rate value of 0.63856 mm/year and specimen An at the 1G welding position has the lowest corrosion rate of 0.058567 mm/year.
first_indexed 2024-04-10T06:20:08Z
format Article
id doaj.art-fb0e1c216aa94ff58f5852f87211ac34
institution Directory Open Access Journal
issn 2405-8440
language English
last_indexed 2024-04-10T06:20:08Z
publishDate 2023-02-01
publisher Elsevier
record_format Article
series Heliyon
spelling doaj.art-fb0e1c216aa94ff58f5852f87211ac342023-03-02T05:01:14ZengElsevierHeliyon2405-84402023-02-0192e13366Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061Danang Priyasudana0Simonne Andrean Crisdion1Poppy Puspitasari2 Triyono3 Jamasri4 Andoko5Diki Dwi Pramono6Department of Mechanical Engineering, Universitas Negeri Malang, IndonesiaDepartment of Mechanical Engineering, Universitas Negeri Malang, IndonesiaDepartment of Mechanical Engineering, Universitas Negeri Malang, Indonesia; Centre of Advanced Material and Renewable Energy, Universitas Negeri Malang, Indonesia; Corresponding author. Department of Mechanical Engineering, Universitas Negeri Malang, Indonesia.Department of Mechanical Engineering, Universitas Negeri Surakarta, IndonesiaDepartment of Mechanical Engineering, Universitas Gajah Mada, IndonesiaDepartment of Mechanical Engineering, Universitas Negeri Malang, IndonesiaDepartment of Mechanical Engineering, Universitas Negeri Malang, IndonesiaFriction Stir Welding (FSW) is a solid-state welding method that has diffusion and different metal structures can blend well. Friction stir welding (FSW) has a weakness, one of which is the lack of flexibility the welding process is only carried out on one side of the plate being welded, so it is not applied on thick materials. Double side friction stir welding is a double working process in which the plate to be welded is subjected to friction from two tools on opposite sides. In the DS-FSW welding process, the dimensions and geometry of the tool and pin greatly affect the quality of the joint. This study to determine the mechanical properties and corrosion rate of Double side friction stir welding aluminum 6061 with variation rotation speed and axis of top and bottom tools. The results of this radiographic test can be seen that specimen 4 welded with variations in speed and tool position has defects in the form of incomplete fusion (IF). The results of microstructural observations showed that the heat caused by the welding process resulted in recrystallization in the form of fine grains in the stirring area and there was no phase change. The highest hardness value in the welding area is specimen B. The largest bending value at the 1G welding positions is specimen D, which is 41.86 MPa with a strain value of 13.23%, while the smallest value at the 4G welding position is specimen A, which is 38.18 MPa with a strain value of 5.03%. The fracture and crack surfaces showed that crack initiation, propagation and material stirring failure occurred in all test specimens, even though the impact test specimen was cut in a small area of Incomplete Fusion, but the test results showed that there was still a surface of the parent metal that had not been stirred. The corrosion test method uses three electrode cells with corrosion media as a substitute for seawater with a salinity of 3.5% NaCl, result of corrosion test is specimen B at the 1G welding position has the highest corrosion rate value of 0.63856 mm/year and specimen An at the 1G welding position has the lowest corrosion rate of 0.058567 mm/year.http://www.sciencedirect.com/science/article/pii/S240584402300573XAluminumFriction stir weldingDouble side friction stir weldingMechanical propertiesCorrosion
spellingShingle Danang Priyasudana
Simonne Andrean Crisdion
Poppy Puspitasari
Triyono
Jamasri
Andoko
Diki Dwi Pramono
Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061
Heliyon
Aluminum
Friction stir welding
Double side friction stir welding
Mechanical properties
Corrosion
title Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061
title_full Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061
title_fullStr Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061
title_full_unstemmed Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061
title_short Double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy AA6061
title_sort double side friction stir welding effect on mechanical properties and corrosion rate of aluminum alloy aa6061
topic Aluminum
Friction stir welding
Double side friction stir welding
Mechanical properties
Corrosion
url http://www.sciencedirect.com/science/article/pii/S240584402300573X
work_keys_str_mv AT danangpriyasudana doublesidefrictionstirweldingeffectonmechanicalpropertiesandcorrosionrateofaluminumalloyaa6061
AT simonneandreancrisdion doublesidefrictionstirweldingeffectonmechanicalpropertiesandcorrosionrateofaluminumalloyaa6061
AT poppypuspitasari doublesidefrictionstirweldingeffectonmechanicalpropertiesandcorrosionrateofaluminumalloyaa6061
AT triyono doublesidefrictionstirweldingeffectonmechanicalpropertiesandcorrosionrateofaluminumalloyaa6061
AT jamasri doublesidefrictionstirweldingeffectonmechanicalpropertiesandcorrosionrateofaluminumalloyaa6061
AT andoko doublesidefrictionstirweldingeffectonmechanicalpropertiesandcorrosionrateofaluminumalloyaa6061
AT dikidwipramono doublesidefrictionstirweldingeffectonmechanicalpropertiesandcorrosionrateofaluminumalloyaa6061