Cooling rates in multipass submerged arc welds
Submerged arc welds using various welding speeds were deposited in groove welds and cooling times between 800-500°C (1472-932°F)were measured for all passes of welds and correlated with the weld features. The objective of the work was to study the effect of the pass number on the cooling rate in a m...
Main Author: | Yeoh, Beng Chai. |
---|---|
Other Authors: | Chandel, R.S |
Format: | Thesis |
Language: | English |
Published: |
2009
|
Subjects: | |
Online Access: | http://hdl.handle.net/10356/19829 |
Similar Items
-
Metal powder addition in submerged arc welds
by: Cheong, Fook Loy.
Published: (2009) -
Submerged arc welding of low-alloy steels
by: Chandel, Roop Singh., et al.
Published: (2008) -
Submerged arc welding of low alloyed steel
by: Lee, Chee Sun.
Published: (2008) -
Metal powder addition in submerged arc welds
by: Chandel, Roop Singh., et al.
Published: (2008) -
Slag detachability from submerged arc welds
by: Oladipupo, Adebisi Oladimeji
Published: (2005)