PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC

Asbuton is a type of natural asphlat that can be found in Buton Island (Asbuton Utilization Guidelines, 2006). Asbuton contains bitumen with variety amount of the bitumen between 10% -40%. Asbuton contains mineral materials, bitumen and water. The number of deposite of asbuton is amounted to 677.247...

Full description

Bibliographic Details
Main Authors: , Galih Pranantya, , Dr. Ir. Latif Budi Suparma, M.Sc.
Format: Thesis
Published: [Yogyakarta] : Universitas Gadjah Mada 2013
Subjects:
ETD
_version_ 1797033914497236992
author , Galih Pranantya
, Dr. Ir. Latif Budi Suparma, M.Sc.
author_facet , Galih Pranantya
, Dr. Ir. Latif Budi Suparma, M.Sc.
author_sort , Galih Pranantya
collection UGM
description Asbuton is a type of natural asphlat that can be found in Buton Island (Asbuton Utilization Guidelines, 2006). Asbuton contains bitumen with variety amount of the bitumen between 10% -40%. Asbuton contains mineral materials, bitumen and water. The number of deposite of asbuton is amounted to 677.247 million ton (Asbuton Utilization Guidelines, 2006). Due to the large number asbuton reserved, it needs to be studied to determine the characteristics of asbuton usage in pavement layer. The aim of this research is to study the durability as one of characteristics of a pavement layer by utilizing BNA blend 75:25 as a binder. Durability testing was conducted to determine the value of durability index of HRS-WC pavement layers by using BNA blend 75:25. The value of durability index by using BNA blend 75:25 subsequently compared to the value of durability index by using asphalt pen.60/70 as a binder. The value of durability index was obtained after 14 days immersing period. The results of this study showed the value of durability index by using BNA blend 75:25 based on RMS and TSR values are 23,46% and 47,38% respectively. Whilst, the value of durability index of HRS-WC mixture by using asphalt pen.60/70 based on RMS and TSR values are 14,84% and 37,50%. The value of durability index by using BNA Blend 75:25 is greater then by using asphalt pen. 60/70 as a binder for pavement, both based on RMS and TSR. It shows that based on the durability point of view the use of asphalt pen.60/70 is better than the use of BNA 75:25 blend as binder in pavement layer.
first_indexed 2024-03-13T23:02:26Z
format Thesis
id oai:generic.eprints.org:123162
institution Universiti Gadjah Mada
last_indexed 2024-03-13T23:02:26Z
publishDate 2013
publisher [Yogyakarta] : Universitas Gadjah Mada
record_format dspace
spelling oai:generic.eprints.org:1231622016-03-04T08:38:14Z https://repository.ugm.ac.id/123162/ PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC , Galih Pranantya , Dr. Ir. Latif Budi Suparma, M.Sc. ETD Asbuton is a type of natural asphlat that can be found in Buton Island (Asbuton Utilization Guidelines, 2006). Asbuton contains bitumen with variety amount of the bitumen between 10% -40%. Asbuton contains mineral materials, bitumen and water. The number of deposite of asbuton is amounted to 677.247 million ton (Asbuton Utilization Guidelines, 2006). Due to the large number asbuton reserved, it needs to be studied to determine the characteristics of asbuton usage in pavement layer. The aim of this research is to study the durability as one of characteristics of a pavement layer by utilizing BNA blend 75:25 as a binder. Durability testing was conducted to determine the value of durability index of HRS-WC pavement layers by using BNA blend 75:25. The value of durability index by using BNA blend 75:25 subsequently compared to the value of durability index by using asphalt pen.60/70 as a binder. The value of durability index was obtained after 14 days immersing period. The results of this study showed the value of durability index by using BNA blend 75:25 based on RMS and TSR values are 23,46% and 47,38% respectively. Whilst, the value of durability index of HRS-WC mixture by using asphalt pen.60/70 based on RMS and TSR values are 14,84% and 37,50%. The value of durability index by using BNA Blend 75:25 is greater then by using asphalt pen. 60/70 as a binder for pavement, both based on RMS and TSR. It shows that based on the durability point of view the use of asphalt pen.60/70 is better than the use of BNA 75:25 blend as binder in pavement layer. [Yogyakarta] : Universitas Gadjah Mada 2013 Thesis NonPeerReviewed , Galih Pranantya and , Dr. Ir. Latif Budi Suparma, M.Sc. (2013) PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC. UNSPECIFIED thesis, UNSPECIFIED. http://etd.ugm.ac.id/index.php?mod=penelitian_detail&sub=PenelitianDetail&act=view&typ=html&buku_id=63273
spellingShingle ETD
, Galih Pranantya
, Dr. Ir. Latif Budi Suparma, M.Sc.
PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC
title PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC
title_full PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC
title_fullStr PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC
title_full_unstemmed PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC
title_short PENGARUH PEMANFAATAN BNA BLEND 75:25 TERHADAP STABILITAS DAN DURABILITAS PADA CAMPURAN HRS-WC
title_sort pengaruh pemanfaatan bna blend 75 25 terhadap stabilitas dan durabilitas pada campuran hrs wc
topic ETD
work_keys_str_mv AT galihpranantya pengaruhpemanfaatanbnablend7525terhadapstabilitasdandurabilitaspadacampuranhrswc
AT drirlatifbudisuparmamsc pengaruhpemanfaatanbnablend7525terhadapstabilitasdandurabilitaspadacampuranhrswc