Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi

Tungsten carbide cobalt, WC-Co composites are essentially aggregates of particle of tungsten carbide bonded with cobalt metal via solid-state sintering. Ultrafine-grained WC-Co composites have potential to replace standard materials for tools and wear parts because of their tremendous mechanical pro...

Full description

Bibliographic Details
Main Author: Azmi, Aidilrizam
Format: Student Project
Language:English
Published: 2017
Subjects:
Online Access:https://ir.uitm.edu.my/id/eprint/35028/1/35028.pdf
_version_ 1825738040394383360
author Azmi, Aidilrizam
author_facet Azmi, Aidilrizam
author_sort Azmi, Aidilrizam
collection UITM
description Tungsten carbide cobalt, WC-Co composites are essentially aggregates of particle of tungsten carbide bonded with cobalt metal via solid-state sintering. Ultrafine-grained WC-Co composites have potential to replace standard materials for tools and wear parts because of their tremendous mechanical properties especially on hardness and toughness. However, one of the crucial aspects in fabrication fine¬grained WC-Co using powder metallurgy route is during sintering stage. Inappropriate sintering temperature may contribute to lower mechanical properties. Lower sintering temperature will lead to incomplete sintering while too high sintering temperature constituting the driving force for the grain growth process. The aim of this investigation was to study the optimum sintering temperature of WC-Co with carbon addition. In this work, ultrafine-grained powder of WC was used and sintering is conducted at liquid-solid-state in gas environment of 95% nitrogen and 5% hydrogen. Samples were fabricated through powder metallurgy route and sintered at three different temperatures which is 1350 °C, 1400 °C and 1450 °C and held for 1 hour. The effect of carbon addition in WC-Co composite towards the mechanical properties; density, hardness, transverse rupture strength, and microstructure formation at varies sintering temperature were examined using standard test procedures. The results signify that the fabricated samples produced higher density and hardness compared to commercial WC-Co cutting tools.
first_indexed 2024-03-06T02:27:33Z
format Student Project
id oai:ir.uitm.edu.my:35028
institution Universiti Teknologi MARA
language English
last_indexed 2024-03-06T02:27:33Z
publishDate 2017
record_format dspace
spelling oai:ir.uitm.edu.my:350282020-10-12T01:47:14Z https://ir.uitm.edu.my/id/eprint/35028/ Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi Azmi, Aidilrizam Machine shops and machine shop practice Machine tools and machining Abrading machinery. Grinding, lapping, etc. Sharpening Tungsten carbide cobalt, WC-Co composites are essentially aggregates of particle of tungsten carbide bonded with cobalt metal via solid-state sintering. Ultrafine-grained WC-Co composites have potential to replace standard materials for tools and wear parts because of their tremendous mechanical properties especially on hardness and toughness. However, one of the crucial aspects in fabrication fine¬grained WC-Co using powder metallurgy route is during sintering stage. Inappropriate sintering temperature may contribute to lower mechanical properties. Lower sintering temperature will lead to incomplete sintering while too high sintering temperature constituting the driving force for the grain growth process. The aim of this investigation was to study the optimum sintering temperature of WC-Co with carbon addition. In this work, ultrafine-grained powder of WC was used and sintering is conducted at liquid-solid-state in gas environment of 95% nitrogen and 5% hydrogen. Samples were fabricated through powder metallurgy route and sintered at three different temperatures which is 1350 °C, 1400 °C and 1450 °C and held for 1 hour. The effect of carbon addition in WC-Co composite towards the mechanical properties; density, hardness, transverse rupture strength, and microstructure formation at varies sintering temperature were examined using standard test procedures. The results signify that the fabricated samples produced higher density and hardness compared to commercial WC-Co cutting tools. 2017-01 Student Project NonPeerReviewed text en https://ir.uitm.edu.my/id/eprint/35028/1/35028.pdf Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi. (2017) [Student Project] (Unpublished)
spellingShingle Machine shops and machine shop practice
Machine tools and machining
Abrading machinery. Grinding, lapping, etc. Sharpening
Azmi, Aidilrizam
Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi
title Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi
title_full Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi
title_fullStr Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi
title_full_unstemmed Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi
title_short Influence of carbon addition on sintering behaviour in ultrafine wc-co Powder / Aidilrizam Azmi
title_sort influence of carbon addition on sintering behaviour in ultrafine wc co powder aidilrizam azmi
topic Machine shops and machine shop practice
Machine tools and machining
Abrading machinery. Grinding, lapping, etc. Sharpening
url https://ir.uitm.edu.my/id/eprint/35028/1/35028.pdf
work_keys_str_mv AT azmiaidilrizam influenceofcarbonadditiononsinteringbehaviourinultrafinewccopowderaidilrizamazmi