High temperature indentation of helium-implanted tungsten
Nanoindentation has been performed on tungsten, unimplanted and helium-implanted to ~600. appm, at temperatures up to 750. °C. The hardening effect of the damage was 0.90. GPa at 50. °C, but is negligible above 450. °C. The hardness value at a given temperature did not change on re-testing after hea...
Prif Awduron: | Gibson, J, Roberts, S, Armstrong, D |
---|---|
Fformat: | Journal article |
Iaith: | English |
Cyhoeddwyd: |
Elsevier
2015
|
Eitemau Tebyg
-
High temperature indentation of helium-implanted tungsten
gan: Gibson, J, et al.
Cyhoeddwyd: (2015) -
Effects of sequential tungsten and helium ion implantation on nano-indentation hardness of tungsten
gan: Armstrong, D, et al.
Cyhoeddwyd: (2013) -
Orientation-dependent indentation response of helium-implanted tungsten
gan: Das, S, et al.
Cyhoeddwyd: (2019) -
Hardening and strain localisation in helium-ion-implanted tungsten
gan: Das, S, et al.
Cyhoeddwyd: (2019) -
The effect of helium implantation on the deformation behaviour of tungsten: X-ray micro-diffraction and nanoindentation
gan: Das, S, et al.
Cyhoeddwyd: (2018)