Crack propagation in fine grained graphites under mode I and mixed-mode loading, as observed in situ by microtomography

Stable crack growth under mode I and mixed-mode loading of two fine grained advanced graphites, SNG742 and T220, has been studied within small (18 mm diameter) specimens of the diametral compression disc geometry to investigate the criterion for crack propagation. Cracks were propagated from a centr...