Removal and Reoccurrence of LLZTO Surface Contaminants under Glovebox Conditions
The reactivity of Li6.4La3Zr1.4Ta0.6O12 (LLZTO) solid electrolytes to form lithio-phobic species such as Li2CO3 on their surface when exposed to trace amounts of H2O and CO2 limits the progress of LLZTO-based solid-state batteries. Various treatments, such as annealing LLZTO within a glovebox or aci...
Main Authors: | Siniscalchi, M, Gibson, JS, Tufnail, J, Swallow, JEN, Lewis, J, Matthews, G, Karagoz, B, van Spronsen, MA, Held, G, Weatherup, RS, Grovenor, CRM, Speller, SC |
---|---|
Format: | Journal article |
Language: | English |
Published: |
American Chemical Society
2024
|
Similar Items
-
Initiation of dendritic failure of LLZTO via sub-surface lithium deposition
by: Siniscalchi, M, et al.
Published: (2024) -
On the relative importance of li bulk diffusivity and interface morphology in determining the stripped capacity of metallic anodes in solid-state batteries
by: Siniscalchi, M, et al.
Published: (2022) -
Robot-Assisted Glovebox Teleoperation for Nuclear Industry
by: Ozan Tokatli, et al.
Published: (2021-07-01) -
On the Surface Modification of LLZTO with LiF via a Gas-Phase Approach and the Characterization of the Interfaces of LiF with LLZTO as Well as PEO+LiTFSI
by: Manuel Donzelli, et al.
Published: (2022-10-01) -
Revealing the role of CO during CO2 hydrogenation on Cu surfaces with in situ soft X-ray spectroscopy
by: Swallow, JEN, et al.
Published: (2023)