Supporting Data - Bulk O-2 formation and Mg displacement explain O-redox in Na0.67Mn0.72Mg0.28O2
Data were collected in PGB labs during 2018-2021
Príomhchruthaitheoir: | Bruce, P |
---|---|
Formáid: | Dataset |
Foilsithe / Cruthaithe: |
University of Oxford
2021
|
Míreanna comhchosúla
Míreanna comhchosúla
-
Bulk O2 formation and Mg displacement explain O-redox in Na0.67Mn0.72Mg0.28O2
de réir: Boivin, E, et al.
Foilsithe / Cruthaithe: (2021) -
Oxygen redox chemistry without excess alkali-metal ions in Na2/3[Mg0.28Mn0.72]O2
de réir: Maitra, U, et al.
Foilsithe / Cruthaithe: (2018) -
Improved oxidation behavior of Hf0.11Al0.20B0.69 in comparison to Hf0.28B0.72 magnetron sputtered thin films
de réir: Pauline Kümmerl, et al.
Foilsithe / Cruthaithe: (2024-09-01) -
Magnetocaloric Effect, Magnetoresistance of Sc<sub>0.28</sub>Ti<sub>0.72</sub>Fe<sub>2</sub>, and Phase Diagrams of Sc<sub>0.28</sub>Ti<sub>0.72</sub>Fe<sub>2−<i>x</i></sub><i>T<sub>x</sub></i> Alloys with <i>T</i> = Mn or Co
de réir: Liting Sun, et al.
Foilsithe / Cruthaithe: (2020-05-01) -
Author Correction: Improved oxidation behavior of Hf0.11Al0.20B0.69 in comparison to Hf0.28B0.72 magnetron sputtered thin films
de réir: Pauline Kümmerl, et al.