Crystal structure of ZnWO(4) scintillator material in the range of 3-1423 K.
The behaviour of the crystal structure of ZnWO(4) was investigated by means of synchrotron and neutron powder diffraction in the range of 3-300 K. Thermal analysis showed the sample's melting around 1486 K upon heating and subsequent solidification at 1442 K upon cooling. Therefore, the structu...
Auteurs principaux: | Trots, D, Senyshyn, A, Vasylechko, L, Niewa, R, Vad, T, Mikhailik, V, Kraus, H |
---|---|
Format: | Journal article |
Langue: | English |
Publié: |
2009
|
Documents similaires
-
Effect of Ca doping on the structure and scintillation properties of ZnWO4
par: Kraus, H, et autres
Publié: (2007) -
Scintillation properties of pure and Ca-doped ZnWO4 crystals
par: Danevich, F, et autres
Publié: (2008) -
ZnWO4 scintillators for cryogenic dark matter experiments
par: Kraus, H, et autres
Publié: (2009) -
Luminescence of CaWO4, CaMoO4, and ZnWO4 scintillating crystals under different excitations
par: Mikhailik, V, et autres
Publié: (2005) -
Multiple photon counting coincidence (MPCC) technique for scintillator characterisation and its application to studies of CaWO4 and ZnWO4 scintillators
par: Kraus, H, et autres
Publié: (2005)