Surface and defect structure of oxide nanowires on SrTiO3.
Processing the SrTiO(3)(001) surface results in the self-assembly of reduced titanate nanowires whose widths are approximately 1 nm. We have imaged these nanowires and their defects at elevated temperatures by atomic resolution scanning tunneling microscopy. The nanowire structure is modeled with de...
Autores principales: | Marshall, MS, Becerra-Toledo, A, Marks, L, Castell, M |
---|---|
Formato: | Journal article |
Lenguaje: | English |
Publicado: |
2011
|
Ejemplares similares
-
Surface and defect structure of oxide nanowires on SrTiO3.
por: Marshall, MS, et al.
Publicado: (2011) -
Surface and Defect Structure of Oxide Nanowires on SrTiO3 (vol 107, 086102, 2011)
por: Marshall, M, et al.
Publicado: (2011) -
Structure and composition of linear TiOx nanostructures on SrTiO3(001)
por: Marshall, M, et al.
Publicado: (2012) -
c(4 × 2) and related structural units on the SrTiO3(001) surface: scanning tunneling microscopy, density functional theory, and atomic structure.
por: Becerra-Toledo, A, et al.
Publicado: (2012) -
Water adsorption on SrTiO3(001): I. Experimental and simulated STM
por: Becerra-Toledo, A, et al.
Publicado: (2012)