Cycle-induced interfacial degradation and transition metal cross-over in LiNi0.8Mn0.1Co0.1O2-graphite cells
<p>Ni-rich lithium nickel manganese cobalt (NMC) oxide cathode materials promise Li-ion batteries with increased energy density and lower cost. However, higher Ni content is accompanied by accelerated degradation and thus poor cycle lifetime, with the underl...
Main Authors: | Bjorklund, E, Xu, C, Dose, W, Sole, C, Thakur, P, Lee, T-L, De Volder, M, Grey, C, Weatherup, RS |
---|---|
Format: | Journal article |
Language: | English |
Published: |
American Chemical Society
2022
|
Similar Items
-
Effects of Degradation on the Thermal Stability LiNi0.8Co0.1Mn0.1O2/Graphite Batteries
by: Takao INOUE, et al.
Published: (2022-11-01) -
Carbonized Polymer Dots Enhancing Interface Stability of LiNi0.8Co0.1Mn0.1O2 Cathodes
by: Lin Li, et al.
Published: (2023-07-01) -
A Three in One Strategy to Achieve Zirconium Doping, Boron Doping, and Interfacial Coating for Stable LiNi0.8Co0.1Mn0.1O2 Cathode
by: Ze Feng, et al.
Published: (2021-01-01) -
Ti4+ Substitution on Structure and Conductivity of LiNi0.8Mn0.1Co(0.1-x)TixO2 as Battery Cathode (x = 0.01, 0.02, and 0.03)
by: Maya Puspitasari Izaak, et al.
Published: (2022-12-01) -
Benchmarking the electrochemical parameters of the LiNi0.8Mn0.1Co0.1O2 positive electrode material for Li-ion batteries
by: Aleksandra A. Savina, et al.
Published: (2023-12-01)