The strength of Al2O3/SiC nanocomposites after grinding and annealing
Alumina matrix nanocomposites containing about 5 vol.% SiC of < 100 nm mean particle size show a substantial increase in strength after machining and annealing. The final strength is controlled by the annealing process and achieves the same level after a coarse machining using 150-grit diamon...
Päätekijät: | Wu, H, Lawrence, C, Roberts, S, Derby, B |
---|---|
Aineistotyyppi: | Conference item |
Julkaistu: |
1998
|
Samankaltaisia teoksia
-
Erosion resistance of hot pressed Al2O3/SiC nanocomposites
Tekijä: Lawrence, C, et al.
Julkaistu: (1998) -
Erosive wear of alumina/SiC nanocomposite ceramics
Tekijä: Lawrence, C, et al.
Julkaistu: (1999) -
Crack healing in an alumina/silicon carbide nanocomposite after grinding and annealing
Tekijä: Wu, H, et al.
Julkaistu: (2000) -
Residual stress distributions around indentations and scratches in polycrystalline Al2O3 and Al2O3/SiC nanocomposites measured using fluorescence probes
Tekijä: Wu, H, et al.
Julkaistu: (2008) -
Wet erosion behaviour of low SiC alumina-SiC nanocomposites
Tekijä: Kara, H, et al.
Julkaistu: (2002)