The role of O2 in O-redox cathodes for Li-ion batteries
The energy density of Li-ion batteries can be improved by storing charge at high voltages through the oxidation of oxide ions in the cathode material. However, oxidising O2- triggers irreversible structural rearrangements in the bulk and an associated loss of the high voltage plateau replacing it wi...
Main Authors: | House, R, Marie, J-J, Pérez-Osorio, MA, Rees, G, Boivin, E, Bruce, PG |
---|---|
Format: | Journal article |
Language: | English |
Published: |
Springer Nature
2021
|
Similar Items
-
Bulk O2 formation and Mg displacement explain O-redox in Na0.67Mn0.72Mg0.28O2
by: Boivin, E, et al.
Published: (2021) -
Covalency does not suppress O2 formation in 4d and 5d Li-rich O-redox cathodes
by: House, R, et al.
Published: (2021) -
Redox chemistry and the role of trapped molecular O2 in li-rich disordered rocksalt oxyfluoride cathodes
by: Sharpe, R, et al.
Published: (2020) -
The role of Ni and Co in suppressing O-loss in Li-rich layered cathodes
by: Boivin, E, et al.
Published: (2020) -
First cycle voltage hysteresis in Li-rich 3d cathodes associated with molecular O2 trapped in the bulk
by: House, RA, et al.
Published: (2020)