Fracture toughness, surface flaw sizes and flaw densities in Al2O3
Surface flaw sizes and flaw densities on polished dense polycrystalline alumina specimens with grain sizes G = 1.2, 3.8 and 14.1 μm were measured using Hertzian indentation. Two surface finishes were studied: well-polished (Syton) and coarse-polished (45 μm diamond paste). Flaw sizes and densities d...
Príomhchruthaitheoirí: | Franco, A, Roberts, S, Warren, P |
---|---|
Formáid: | Journal article |
Teanga: | English |
Foilsithe / Cruthaithe: |
1997
|
Míreanna comhchosúla
Míreanna comhchosúla
-
Progress in flaw growth and fracture toughness testing /
de réir: National Symposium on Fracture Mechanics (6th : Philadelphia, 1972), et al.
Foilsithe / Cruthaithe: (1973) -
SURFACE FLAW DISTRIBUTIONS IN BRITTLE MATERIALS AND HERTZIAN FRACTURE
de réir: Warren, P, et al.
Foilsithe / Cruthaithe: (1994) -
Indentation fracture toughness and surface flaw analysis of sintered alumina/SiC nanocomposites
de réir: Anya, C, et al.
Foilsithe / Cruthaithe: (1996) -
Flaw growth and fracture
de réir: National Symposium on Fracture Mechanics (10th : 1976 : Philadelphia, Pa.), et al.
Foilsithe / Cruthaithe: (1977) -
THE PROPULSION OF SURFACE FLAWS BY ELASTIC INDENTATION TESTING
de réir: Dai, D, et al.
Foilsithe / Cruthaithe: (1995)